Real applications of Kezhibo PVC coated fabric across logistics, architecture, events and industry. Each case links to the product and standards used.
Logistics — European curtainsider fleet
A European haulier needed side curtains that stay flexible in winter and meet EN 12641-2. We supplied 650 gsm PVC truck curtain fabric, cold-flexible to -30℃, welded to trailer dimensions. Result: clean folding, no fold-line cracking, printable for fleet livery. → Truck curtain fabric
Architecture — tensile canopy project
A transport-hub canopy used PVDF-coated PVC architectural membrane (950 gsm, tensile 6000 N/5cm) for a 15–20 year, self-cleaning roof. B1 / EN 13501-1 fire rating satisfied local code. → Architectural membrane
Events — modular marquee programme
An event-rental company standardized on 850 gsm flame-retardant tent fabric (NFPA 701 / CPAI-84) for marquees and pagodas, with printed branding. → Tent & event fabric
Industry — welding-bay protection
A fabrication plant installed flame-retardant welding curtains (450 gsm) to screen sparks, spatter and UV glare across multiple bays. → Industrial PVC fabric
Advertising — large-format billboard rollout
A signage contractor used knife-coated PVC banner (550 gsm) for 1–3 year outdoor billboards, wide-format and color-fast. → Banner & signage fabric
Your project next
Get a quote or request a sample and tell us your application.
Note: customer names/logos shown only with permission. Replace placeholders with approved references before publishing.