Kezhibo supplies PVC fabric for construction and architecture — tensile membrane for permanent roofs and facades, plus temporary enclosure and site-covering fabric. The membrane grades combine structural strength, controlled translucency and 15–20 year PVDF weather life.

Solutions

Application Product Spec
Tensile roof / facade Architectural membrane 650–1050 gsm, PVDF
Canopy / awning Awning fabric 440–650 gsm, UV-stable
Temporary enclosure PVC tarpaulin 650–900 gsm
Site / scaffold cover PVC tarpaulin 510–650 gsm

Why Kezhibo for projects

  • Structural strength – tensile 4000–7000 N/5cm.
  • Fire rated – B1 / EN 13501-1.
  • Self-cleaning PVDF – 15–20 year life.
  • Project support – patterning, welding and QA.

Applications

Stadium and arena roofs, station and airport canopies, commercial facades, car-park shades, temporary site enclosure, scaffold wrapping and construction covers.

Standards

EN 13501-1, DIN 4102 B1, REACH. See Certifications.

Project enquiry

Request a sample or get a quote with span, load and finish.

FAQ

PVDF-coated PVC membrane (850–1050 gsm) — 15–20 year life, self-cleaning.

Yes — B1 / EN 13501-1 on request.

Yes, we assist with patterning and welding for tensile projects.

Yes — 650–900 gsm PVC tarpaulin for site enclosure.