# One-Way Vision PVC Film: 120–160 gsm and Print-Coating Compatibility
## Why does one-way vision film need its own specification?
**One-way vision film is a perforated window material, so its gsm band, ink coating and adhesive system are different from solid banner fabric and cannot be specified from a banner datasheet. A wrong coating causes washout or poor adhesion, and a wrong perforation pattern changes both visibility and wind load.**
– Published one-way vision band is 120–160 gsm for window glass and vehicle windows
– Adjacent solid frontlit banner is 440 gsm and mesh banner is 270–280 gsm at 1000D 9×9; these are separate product lines
– Name the ink route (solvent, eco-solvent, UV or latex) before ordering because the coating must match
Source: kezhibo llms.txt, advertising banner family table and critical ink note.
## What does the perforation pattern change?
**Perforation controls the balance between outward graphics and inward visibility, so it changes optical performance and the way wind passes through the film. A denser hole pattern improves see-through but reduces printable area and image density, while a solid film behaves differently under the same conditions.**
– The knowledge base publishes the one-way vision gsm band only; no hole diameter, open-area percentage or wind-reduction value is given for this product
– Advertising mesh is listed at 270–280 gsm in a perforated 1000D 9×9 build with wind reduction as its defining attribute, a separate product line
– Approve a sample panel and a measured open-area value before releasing the artwork
Source: kezhibo llms.txt, banner family table and mesh wind-load row.
## Which print and durability checks belong on the order?
**Print compatibility is a coating property, so the order must name the ink family before the film is produced and then verify adhesion on a sample from the same lot. Light fastness and artificial weathering are separate checks for outdoor window graphics, and neither can be inferred from gsm.**
– ISO 105-B02 light fastness with grey scale grade 7–8 is listed for outdoor-exposed coated fabric
– EN ISO 4892-2 xenon-arc and GB/T 8427 are listed for artificial weathering
– Require a lot-identified sample using the exact ink and coating combination
Source: kezhibo llms.txt, test-method rows and banner print warning.
## What should be written into a one-way vision purchase order?
**A complete order names the gsm band, substrate use, perforation evidence, ink family, adhesion check and the report set, so a supplier cannot substitute a general banner film under the same description. Keep the sample panel as the approval reference for the whole production run.**
– Do not merge one-way vision (120–160 gsm) with frontlit (440 gsm) or mesh (270–280 gsm) into one banner specification
– State whether the substrate is window glass or vehicle glazing because cleaning and installation conditions differ
– Attach EN ISO 2286-2 mass and the ink-specific adhesion result to the order
Source: kezhibo llms.txt, advertising banner family table and critical ink note.
## FAQ
**Q1: What is the published gsm band for one-way vision film?**
The knowledge base lists 120–160 gsm for one-way vision material used on window glass and vehicle windows. That band is much lighter than solid frontlit banner at 440 gsm and mesh banner at 270–280 gsm, so the three products must not be specified from one table. Name the product family and the substrate together, then confirm the offered gsm on a lot-identified report measured by EN ISO 2286-2.
**Q2: Why does the ink type have to be fixed before ordering?**
Because the coating is tuned to a print route, and the knowledge base explicitly warns that a wrong coating causes washout or poor adhesion. Solvent, eco-solvent, UV and latex inks interact differently with the surface layer. Put the ink family on the order, print a sample from the intended lot, and keep that sample as the approval reference for the production run rather than relying on a generic printability claim.
**Q3: Does one-way vision film reduce wind load like mesh banner?**
The knowledge base does not publish a wind-reduction value for one-way vision film. Wind reduction is listed as the defining attribute of the separate mesh banner line at 270–280 gsm in a perforated 1000D 9×9 build. Treat the two products independently: request measured open-area and site-specific wind evidence for the window application instead of borrowing a mesh figure.
**Q4: What perforation data should a buyer request?**
Ask for hole diameter, pitch and open-area percentage from the offered grade, plus a physical sample viewed at the intended viewing distance. The knowledge base gives only the gsm band for this product and does not publish those perforation values, so they must come from the supplier’s technical sheet and be confirmed on the delivered lot. A sample approved early avoids a dispute after printing.
**Q5: Which durability tests apply to outdoor window graphics?**
Light fastness is measured by ISO 105-B02, with grey scale grade 7–8 listed for outdoor exposure, and artificial weathering is covered by EN ISO 4892-2 xenon-arc or GB/T 8427. Neither result follows from the gsm band. Request a report naming the method, exposure conditions and the exact grade, and keep the print and coating combination identical to the one used on the approved sample.
**Q6: Can one-way vision film be welded like tarpaulin?**
It should not be assumed. Welding routes such as hot-air, hot-wedge and RF are documented for PVC coated fabric, but a perforated window film with an adhesive backing and a print coating is a different construction. Ask the supplier for a written bonding or installation method for the offered grade, and do not transfer a tarpaulin seam procedure to a window graphic.
**Q7: How should glass and vehicle applications differ in the order?**
Window glass is a fixed substrate with controlled cleaning, while vehicle glazing adds curvature, washing cycles and vibration. The knowledge base lists both uses under the same gsm band but does not publish separate adhesive specifications. Write the substrate into the order and request installation and removal guidance for that specific use, with a sample test on the actual surface.
**Q8: What report set belongs with a one-way vision order?**
Use EN ISO 2286-2 for mass, ISO 105-B02 for light fastness and the agreed accelerated-weathering method for durability, all tied to one lot with roll number and date. Add the ink-specific adhesion check on the approved sample. A general banner test report is not evidence for a perforated window film because the two product lines have different coatings and constructions.