In mid-November 2026 the Chinese PVC paste resin market is broadly flat with a few lower quotes: glove-grade microsuspension at CNY 7,100–7,300 per tonne, bulk-grade microsuspension at CNY 7,100–7,400, and seed-emulsion grade at CNY 6,100–6,600. Industry utilisation stands at 74.50% with weekly output of 25,815 tonnes — but carbide-based lines are running at 83.42% while ethylene-based lines manage only 61.81%. For coated fabric buyers, the message is that costs are soft in aggregate yet sharply divided by route. Which grade you actually buy matters more than whether paste resin went up or down.
First, identify which paste resin you are quoting
PVC paste resin is a branch of PVC resin used mainly in artificial leather, flooring, toys and coated textiles. A listing on the 100ppi commodity portal dated 2026-11-06 describes a product compliant with GB/T 15592-2008, purity at least 99%, K value 65–75 and viscosity 2,000–8,000 mPa·s, packed in 20 kg bags. Two variables are routinely overlooked:
- Polymerisation route — microsuspension and seed emulsion differ in both price and application, with microsuspension generally quoted higher;
- Grade by use — glove grade and bulk grade are both microsuspension but target different specifications and cannot be compared on one price.
Mysteel, citing Longzhong Consultancy for 2026-11-17, gives Shandong quotes of CNY 7,100–7,300 for glove-grade microsuspension, CNY 7,100–7,400 for bulk microsuspension and CNY 6,100–6,600 for bulk seed emulsion. Hebei seed emulsion fell further to CNY 6,050–6,550 on 11-18, while Zhejiang was reported stable on the same day. These are regional spot quotes, not a national average, so state delivery point and settlement terms in every enquiry.
Supply side: plant moves carry more signal than the average
Device news from early to mid-November explains why no single trend has taken hold:
- Jiangsu Kangning Chemical’s 100,000 t/y line stopped around 11-13; grades P450, P440, 1069 and 13 had not been produced;
- Shenyang Chemical’s 220,000 t/y line runs normally, with glove grade PSH-30 at CNY 7,450 ex-works and bulk grade PSM-31 at CNY 7,400;
- Inner Mongolia Chenhongli’s 80,000 t/y line runs normally, bulk 125 and glove 155 both delivered at CNY 7,700;
- Jining Zhongyin’s 40,000 t/y line has been under maintenance since early September, with P440 and P450 at CNY 7,000;
- Shandong Langhui’s 140,000 t/y line is in normal production.
Set the running capacity against the stopped capacity and the 74.50% utilisation reported by Longzhong on 11-18 makes sense: ethylene-based enterprises at 61.81%, carbide-based at 83.42%. That split maps directly onto cost pressure for purchased ethylene. The 11-13 morning note had already flagged that vinyl chloride prices were edging up and ethylene-route cost pressure was increasing.
Cost transmission: how far away coated fabric really is
On 11-12, carbide in Wuhai was CNY 2,550 per tonne and vinyl chloride in Jiangsu CNY 5,650. The morning note judged that carbide had upward potential from orderly power use in Inner Mongolia and restarts in Ningxia, but limited room. That chain runs upstream to carbide and ethylene, and only downstream to paste resin, plasticiser, PVC coated fabric and finished goods.
The distance needs to be stated honestly. Paste resin spot price is not the delivered cost of coated fabric. The fabric also carries base cloth, plasticiser, stabilisers, flame retardants, coating conversion and waste. Consider a second 100ppi quote on 11-06: Wuhan Hengjiu offered premium-grade paste resin at CNY 16,500 per tonne — a small-lot, service-inclusive market quote, not the same basis as the CNY 7,000-class bulk transactions tracked by Longzhong. Mixing the two produces a completely wrong cost picture.
The same applies to the Vinnolit import quotes on Baidu Ai Caigou from October, which sit at CNY 65–75 per kilogramme for branded small orders, while Formosa Plastics PR-415 lists at CNY 10.8–11. Those pages help screen brands and specifications; they are not a price benchmark.
Three practical moves for coated fabric buyers
- Lock the route and grade in the enquiry. Write bulk microsuspension grade into the RFQ instead of just paste resin. In November the gap between microsuspension and seed emulsion was roughly CNY 1,000 per tonne; without a shared basis, quotes cannot be compared.
- Use utilisation and plant moves to time purchases. At 74.50% utilisation and 25,815 tonnes weekly, supply is not tight. But if your grade comes from a stopped line, lead-time risk diverges from the market average.
- Leave room for price adjustment. The market rose CNY 50–100 on 11-03 and 11-04, then returned to flat with isolated cuts. In a short cycle, locking volume is safer than locking price.
One longer-term variable is standards. GB/T 15592-2008 remains the reference printed on many supplier pages; coated fabric exported to Europe must additionally consider REACH and SVHC, a separate logic from domestic spot prices. Cheaper feedstock does not automatically mean lower compliance cost for the finished fabric.
How to read this market
Here is the one-sentence summary of mid-November: supply is not tight, prices are flat, and the two production routes are diverging. The opportunity for downstream buyers is not in guessing the next move but in specifying grade, route, delivery point and settlement terms so that quotes become comparable. Figures here come from public 100ppi and Mysteel pages citing Longzhong, dated 2026-11-06 to 2026-11-18. They are market information, not a purchase commitment; actual transactions follow supplier contracts.
Frequently asked questions
Why can quotes for the same paste resin more than double?
Because the basis differs. Bulk microsuspension sits at CNY 7,100–7,400 per tonne, seed emulsion at CNY 6,050–6,600, small-lot premium-grade quotes reach CNY 16,500, and branded retail lots hit CNY 65–75 per kilogramme. Polymerisation route, grade, minimum order and delivery service all change the number. Compare like with like.
If carbide prices rise, must coated fabric follow immediately?
Not necessarily. Between carbide and coated fabric sit paste resin, plasticiser, base cloth and conversion, so transmission lags. On 11-12 carbide in Wuhai was CNY 2,550, yet Longzhong still judged further carbide gains limited and the paste resin market broadly stable.
Is 74.50% utilisation high or low?
Neutral in aggregate, but the structure matters: carbide-based at 83.42% versus ethylene-based at 61.81%. Buyers should check whether the plant behind their specific grade is running, rather than relying on the industry average.
Sources:
Mysteel: PVC paste resin market flash (2026-11-13)
Mysteel: PVC paste resin price flash, updated 2026-11-19
100ppi: PVC paste resin quotation update (2026-11-06)
100ppi: PVC paste resin quotation detail (2026-11-06)
Baidu Ai Caigou: PVC paste resin brand quotes (2026-10)