Skip to content

REACH Entry 78 Microplastics: EU 2026/1168 and PVC Coated Fabric Exemptions

November 6, 2026 kezhibo News
Tensile test machine testing coated fabric in the laboratory

TL;DR: Commission Regulation (EU) 2026/1168, published in the Official Journal on 2 June 2026, tightens the “permanently incorporated into a solid matrix” exemption in REACH Annex XVII Entry 78 — coated-fabric compounders lose that route whenever the product’s intended final-use duration is less than 1 year, and affected formulations must be substituted or adjusted by 22 June 2028, according to the WTO/FTA Consultation Network briefing published by CCEECCIC on 9 June 2026. A normal continuous PVC coating on a woven polyester scrim is generally not an “intentionally added synthetic polymer microparticle” in the sense of Entry 78, but the burden of demonstrating that now sits squarely with the supplier. Products that continue to rely on any exemption must still meet REACH information-passing, labelling and annual reporting obligations to the European Chemicals Agency (ECHA), per the same briefing.

What exactly did Regulation (EU) 2026/1168 change in REACH Annex XVII Entry 78?

Start with the instrument it corrects. According to Intertek China’s overview of the EU microplastics ban, Commission Regulation (EU) 2023/2055 added Entry 78 to Annex XVII of REACH Regulation (EC) No 1907/2006, restricting intentionally added synthetic polymer microparticles (SPM) for all uses unless exempted, with application from 17 October 2023 except for products granted transitional periods. The European Commission’s Microplastics page confirms the restriction on intentionally added microplastics was adopted in 2023. On 31 March 2025 the Commission published a comprehensive explanatory guide for (EU) 2023/2055, according to China’s MOFCOM WTO/TBT notification portal in its 17 April 2025 notice; the guide names cosmetics, detergents, fertilisers and medical devices among targeted categories, states the aim of reducing unintentional release of persistent, non-biodegradable particles, and notes core provisions were already in force under staged transitions.

Regulation (EU) 2026/1168 does not rewrite that framework. According to the WTO/FTA Consultation Network briefing published by CCEECCIC on 9 June 2026, the Commission published it in the Official Journal on 2 June 2026 to correct legal-wording ambiguities found during implementation of (EU) 2023/2055, without changing the overall direction of microplastics reduction. Its three core changes are narrow but operationally significant.

Three corrections, one unchanged direction

  • Medicinal products: the exemption is clarified to cover clinical trials and related pre-clinical testing.
  • Research and development: a new exemption is added for product and process orientated research and development (PPORD).
  • Solid matrix: the “permanently incorporated into a solid matrix” exemption is tightened.

For a coated-fabric producer, the first two changes barely touch commercial rolls; the third is the one that reopens formulation files. The same CCEECCIC briefing is explicit that exempted products continuing to rely on an exemption still must fulfil REACH information-passing, labelling and annual reporting obligations to ECHA — so even a successful exemption claim is not a documentation-free outcome. For the wider regulatory frame, see REACH compliance for PVC coated fabrics in 2026.

Which coated-fabric uses lose the “permanently incorporated into a solid matrix” exemption?

The tightening is a duration test, not a chemistry ban. According to the CCEECCIC briefing, building materials, coatings, electronic encapsulation and composites lose the solid-matrix exemption if the intended final-use duration is less than 1 year; examples given are temporary protective coatings, quick-release composites, short-life industrial moulds and curing agents, and affected companies must complete formulation substitution or adjustment by 22 June 2028. For coated fabrics the dividing line is the finished article’s intended service life.

The less-than-one-year test

Read “permanently” as a question about the finished article’s design life. A protective layer intended to be peeled off within a single season, a release liner on a short-run tool, or a sacrificial film used only during installation all fall on the wrong side of the line if they carry intentionally added polymer micro-powders. A temporary building membrane specified for one construction phase is the archetype buyers should re-examine first. Permanent architectural membranes are not caught by the duration test, though they still owe the supplier-side proof below.

Where micro-powders enter a coating formulation

Entry 78 concerns intentionally added synthetic polymer microparticles. In PVC compounding the relevant inputs are deliberate particulate additives: polymer-based matting agents used to knock back gloss, texturising powders that build a dry or grain-like hand, microbead-type fillers that control slip and spacing, and some anti-blocking or tactile additives supplied as fine polymer powders. Each is a discrete particle intentionally added at the mixing stage, and each must be identifiable by polymer identity and particle size. Where those powders are present and the finished article is short-lived, the solid-matrix route is no longer available after 2 June 2026, with substitution required by 22 June 2028 per the CCEECCIC briefing.

Is a standard PVC coating on woven polyester scrim an intentionally added microplastic?

Usually, no — and this distinction matters more than any single deadline. A conventional PVC coated fabric is made by applying a continuous plastisol or compound layer onto a woven polyester scrim through a knife-coating or calendering line, then fusing it into a coherent solid film. In that finished state the polymer is a continuous matrix, not a population of discrete particles intentionally added as particles. Entry 78, as described by Intertek China, restricts intentionally added synthetic polymer microparticles; it is not a blanket ban on polymer films. A versatile industrial PVC coated membrane produced as a continuous layer therefore generally sits outside the particle definition, provided no particulate polymer additive is deliberately introduced.

That “provided” is the whole compliance problem. The restriction turns on what the compounder intentionally adds, not on what a finished roll looks like, and the burden of demonstrating the absence of intentionally added SPM sits with the supplier; the answer lives in the formulation record. Where a compounder does add polymer micro-powders, the question becomes whether those particles are “permanently incorporated into a solid matrix” during use — precisely the exemption that 2026/1168 narrowed. For a permanent article with a continuous coating and no particulate additive, nothing changed on 2 June 2026; for a short-life article carrying micro-powders, the ground shifted.

Generic engineering note: knife-coating and calendering both produce continuous layers, not discrete particles. This is process description, not a regulatory classification.

What is the compliance timeline from 2023 to the 2028 substitution deadline?

Each date below comes from a supplied verified source; the 2026 amendment is a wording correction, not a reset of the clock.

Date Milestone Verified source
27 September 2023 Commission Regulation (EU) 2023/2055 published, adding Entry 78 to REACH Annex XVII European Commission Microplastics page and Intertek China
17 October 2023 Entry 78 restriction applies, with transitional periods for certain products Intertek China
31 March 2025 European Commission publishes comprehensive explanatory guide for (EU) 2023/2055 China MOFCOM WTO/TBT notification portal, 17 April 2025 notice
2 June 2026 Regulation (EU) 2026/1168 published in the Official Journal, amending Entry 78 WTO/FTA Consultation Network via CCEECCIC, 9 June 2026 briefing
22 June 2028 Deadline for formulation substitution or adjustment for products losing the solid-matrix exemption WTO/FTA Consultation Network via CCEECCIC

Read the sequence carefully: the 17 October 2023 application date and staged transitions are unchanged; 2026/1168 adds a clarification plus a future substitution backstop. The 22 June 2028 date is a formulation deadline for affected products, not a general sell-through date. The practical trigger is each article’s intended service-life declaration.

How should buyers classify coated-fabric use cases against the exemption routes?

The matrix below is a triage tool, not a legal determination. It applies the two filters that matter after 2 June 2026: whether an intentionally added SPM particle is present, and whether the intended final-use duration clears 1 year. A PVC truck side curtain in long-haul service and a sacrificial installation film sit at opposite ends of that grid even when they come off the same coating line.

Coated-fabric use case Likely exemption route Does 2026/1168 change it? Evidence the supplier must hold
Permanent architectural membrane, continuous PVC coating, no particulate polymer additive Outside Entry 78 scope — no intentionally added SPM particle No, provided no micro-powder additives and service life well beyond 1 year Written SPM statement, additive inventory, intended service-life declaration
Permanent truck side curtain, multi-year service Outside Entry 78 scope, or solid-matrix exemption if particulate additives are present No change to the duration test; exemption paperwork still required if a route is claimed Service-life declaration, additive inventory with particle size and polymer identity, annual ECHA reporting reference
Temporary protective film, intended life under 1 year Previously solid-matrix exemption; now lost where micro-powders are intentionally added Yes — the less-than-1-year condition removes the exemption Reformulation or substitution record by 22 June 2028, ECHA information-passing, labelling and annual reporting reference
Short-life mould release layer, intended life under 1 year Previously solid-matrix exemption; now lost Yes — short-life industrial moulds are named among affected examples Substitution evidence, intended service-life declaration, REACH SDS Section 3/15 alignment
R&D / PPORD samples New PPORD exemption added by 2026/1168 Yes — a new route is available for product and process orientated research and development PPORD documentation, ECHA information-passing, labelling and annual reporting reference

For the permanent rows, “no change” is conditional on the supplier proving no intentionally added polymer microparticle is present. For the PPORD row, the CCEECCIC briefing is clear that exempted products still owe the full set of ECHA obligations; a PPORD claim is a reporting posture, not silence.

What documentation should an importer demand in the RFQ?

The 2026 amendment is, in practice, a documentation event. The CCEECCIC briefing advises affected companies to re-audit compliance files, keep written proof of exemption applicability, start supply-chain communication now and watch the transition deadline. Translate that into five concrete line items for the RFQ and the supplier quality agreement.

  • Written SPM statement. A signed declaration per grade stating whether the formulation contains any intentionally added synthetic polymer microparticle under Entry 78. Ask per grade, not per company.
  • Intended service life declaration. A numeric written intended final-use duration for the specific article; this field decides the less-than-1-year test, and a vague “durable” is not evidence.
  • Additive inventory with particle size and polymer identity. A full list of particulate additives — matting agents, texturising powders, microbead-type fillers, anti-blocking and tactile additives — with polymer identity and particle-size data.
  • Annual ECHA reporting reference. Where an exemption is claimed, the reference for the REACH information-passing, labelling and annual reporting obligations to the European Chemicals Agency that the CCEECCIC briefing says continue to apply.
  • REACH SDS Section 3/15 alignment. Confirm Section 3 (composition) and Section 15 (regulatory information) of the safety data sheet match the SPM statement and exemption claim; contradictions are the fastest route to a detained shipment.

Ask for the same pack in the RFQ, at contract review and at any formulation-change notice, since a change of matting-agent supplier can silently change the particle picture. Substance-level records are becoming a standing requirement: tcworld magazine notes that ESPR (EU) 2024/1781 requires information on substances of concern and environmental impact and that the Construction Products Regulation (EU) 2024/3110 applies from 8 January 2026. For adjacent EU chemical limits, see our 2026 EU coated-fabric chemical-rules overview.

What should coated-fabric buyers do before the 22 June 2028 deadline?

Four actions, in order. First, segment the catalogue by intended service life: flag every SKU with a declared or implied life under 1 year that carries particulate polymer additives. Second, re-audit compliance files against the three 2026/1168 changes and keep written proof of whichever exemption route each grade relies on — the CCEECCIC briefing specifically advises re-auditing files and retaining written proof. Third, open supply-chain communication now, not in 2028: ask compounders for polymer identity and particle-size data behind every matting or texturising powder. Fourth, diarise 22 June 2028 as the substitution backstop and confirm any continuing exemption claim is matched by ECHA information-passing, labelling and annual reporting.

Where substitution is needed, treat it as a specification exercise rather than a drop-in swap: removing a polymer micro-powder matting agent changes gloss, hand and anti-block behaviour, so the replacement must be validated on the same coating line against the same weld and adhesion requirements. Some buyers use the reformulation window to review eco-friendly PVC coated fabric solutions and the recyclable tarpaulin design routes examined in our 2026 circular-economy analysis. Neither route removes the REACH obligation; both change what the supplier must document.

One caveat, stated plainly: this article is technical compliance information for procurement and specification teams, not legal advice. Entry 78 classification depends on the exact formulation and intended use of a specific article; qualified regulatory counsel should confirm the final determination before goods are placed on the EU market.

Where do these figures come from?