ISO 6940:2026, Edition 3, was published on 13 May 2026 with an English correction in June, replacing ISO 6940:2004 after twenty-two years. It measures the ease of ignition of vertically oriented textile specimens exposed to a small defined flame, and its scope explicitly covers coated, quilted, multilayered and sandwich constructions — language that pulls PVC-coated fabric, tarpaulins, tent fabric and outdoor blinds straight into its orbit. Germany adopted it as DIN EN ISO 6940:2026-10 in October 2026, superseding DIN EN ISO 6940:2004-06.
What actually changed
According to the ISO record, ISO 6940:2026 is Edition 3, published in May 2026, 15 pages, developed by ISO/TC 38 with ICS classifications 13.220.40 and 59.080.30; the 2004 edition is withdrawn (https://iso.org/standard/90367.html). A corrected English version appeared in June 2026. The German edition was published in October 2026 at 26 pages and explicitly replaces the 2004-06 version (https://www.dinmedia.de/en/standard/din-en-iso-6940/402987804). Italy’s UNI EN ISO 6940:2026 carries an implementation date of 2 July 2026 (https://plusstd.com/standard/1195239589/uni-en-iso-6940-2026).
One misconception needs clearing up: 6940 is a method standard, not a classification standard. It defines how to test and how to judge whether a specimen ignites; it does not issue a pass/fail grade. Classification belongs to a separate system such as EN 13501-1 fire performance classes. Writing a method standard into a contract without agreeing a class leaves the same argument at acceptance.
What 6940 measures, and what 6941 measures
The full title of ISO 6940 is the determination of ease of ignition of vertically oriented specimens: will the fabric catch, and how quickly, under a defined small flame? The companion EN ISO 6941-2026 measures flame spread properties of vertically oriented specimens: once lit, how fast does the flame travel? They address different halves of the same risk. A coated fabric that resists ignition but spreads flame rapidly would look acceptable if only 6940 were run (https://m.book118.com/html/2026/1102/6234045024012235.shtm).
The 2026 edition explicitly covers single- or multi-component textile forms, listing coated, quilted, multilayered and sandwich constructions (https://iso.org/standard/90367.html). For coated fabrics that matters: the test piece is the finished structure, not the stripped base cloth. A flammable scrim with a fire-resistant coating, or a coating that loses performance once damaged, is only characterised honestly when the finished product is tested.
Where this touches coated-fabric products
Outdoor blind fabric is a clear case. Industry guidance notes that PVC-coated polyester, glass fibre and acrylic — the three common zip-blind fabrics — each require fire documentation to answer three questions: which report, which specimen was tested, and which installation method was used. Grade claims detached from a specific material are meaningless, because performance depends on the base yarn, the coating, the weight and the construction together (https://worldwidetradex.com/zh/supply/horeca-zip-blinds/fire-and-compliance). The same logic applies to tent fabric, hall fabric and printed banner material.
End use also changes the obligation. Coated fabric used as upholstery in the UK must meet the cigarette and match tests of the Furniture and Furnishings (Fire) (Safety) Regulations 1988; fabric for marquees, signage or public buildings is normally governed by separate flame-retardant standards, so grade must match application (https://camchinabridge.co.uk/zh/guides/sourcing-pvc-and-pu-coated-fabrics-from-china). A single 6940 report does not satisfy all of these.
How to check a test report
Other standards in common use for coated fabric include FZ/T 64017-2019, ISO 4674:2016 for physical tests, ISO 14116:2015 for limited flame spread materials and EN ISO 11612:2015, with typical tests covering coating adhesion, hydrostatic resistance, moisture permeability, colour fastness, formaldehyde and pH, flame behaviour and UV resistance (http://www.cma-cert.cn/jc/5626.html). When reviewing a report, confirm four things:
- The standard number and edition — ISO 6940:2026, not the withdrawn 2004 version.
- That the specimen is the exact coated structure and weight ordered, with the coating included.
- Specimen direction and conditioning, since coated fabrics are strongly directional.
- Installation and edge treatment — cut glass yarns or heat-sealed edges can change the result.
FAQ
Is ISO 6940:2026 a flame-retardant grade?
No. It is a method for measuring ease of ignition of vertically oriented specimens, defining procedure and judgement but no class. Grades are normally set under EN 13501-1 or the relevant local building code.
Can a 2024 report to ISO 6940:2004 still be used?
The 2004 edition has been replaced by Edition 3. Whether an older report is accepted depends on the authority, insurer or contract edition specified; new projects should request retesting to the current edition or a documented equivalence statement.
Should the base fabric or the finished coated fabric be tested?
The finished structure. The 2026 edition explicitly includes coated, multilayer and sandwich constructions because flame behaviour comes from the base fabric and coating together; testing the base cloth alone can mislead selection.