The short answer

In July 2026 Belgian technical-textile group Sioen, through its New Zealand distributor W Wiggins, launched Aqualite D2360, a lightweight dual-coated PVC technical textile built for boat covers and yachting enclosures. It weighs just 360 g/m2, comes 218 cm wide on 50 m rolls, uses a 280 dtex all-polyester base cloth and carries up to a 10-year warranty. A special boat embossing gives a subtle leather look, while UV stabilization and anti-bacterial treatment fight sunlight degradation and mould in marine environments.

Why a light boat-cover fabric matters

Power-boat and sailing covers have long faced a trade-off: too heavy to handle, too thin to last. Aqualite D2360 keeps mass at 360 g/m2 yet posts tear strength of 1300/1300 N/5cm and tensile of 70/60 N in the supplier’s data, with a temperature range of minus 40 to plus 70 C and light fastness rated 7 to 8 with a 5-year warranty (the distributor page also lists 10 years). For enclosures that are taken down and put up often, the weight saving is real in handling and storage.

Specifications at a glance

  • Weight 360 g/m2; width 218 cm; roll length 50 m
  • Base cloth 280 dtex polyester 100 percent; coating PVC 100 percent
  • Finish embossed leather pattern, semi-dull lacquer
  • Tear strength warp/weft 1300/1300 N/5cm; tensile warp/weft 70/60 N
  • Adhesion 60 N/5cm; temperature range minus 40 to plus 70 C
  • UV stabilized 7 to 8 light fastness; anti-bacterial, mould and mildew resistant

How it differs from heavy marine canvas

Conventional marine canvas sits in the 450 to 1500 g/m2 range for long outdoor life and heavy mechanical load. Aqualite D2360 is positioned as a light, professional, easy-handling cover and enclosure fabric, trading some mass for embossed looks and anti-bacterial protection. It is not a heavy-duty work cloth but a细分 segment balancing appearance, feel and weight, sitting in a product ladder with Sioen’s Glamping B8176 (650 g/m2 flame retardant) and B6353 foam-insulated acoustic PVC.

Care and selection

  • Prioritize it for boat covers, yacht enclosures and light outdoor covers; pick a heavier grade for long-term heavy load or high-abrasion use.
  • Clean only with warm soapy water and a soft brush; no solvents, abrasives or dry cleaning.
  • Remove mildew with a cold 4 percent chlorine household bleach solution at one part to four of water, then rinse thoroughly.
  • Inspect on delivery within 10 days; later claims are treated as acceptance.

Frequently asked questions

Q: At 360 g/m2, is it tough enough for a boat cover?
A: Tear strength still reaches 1300 N/5cm with UV stabilization and anti-bacterial treatment, suiting covers and enclosures that are frequently handled, but heavy long-term abrasion needs a heavier grade.

Q: How do I choose between Aqualite D2360 and heavy marine canvas?
A: By use intensity. For frequently handled, good-looking yacht covers choose it; for long outdoor heavy load and mechanical stress choose 450 to 1500 g/m2 heavy fabric.

Q: Can this PVC fabric be machine or dry washed?
A: No. Use only warm soapy water and a soft brush; avoid solvents, abrasives and dry cleaning, and treat mildew with diluted bleach.

Sources

The New Zealand distributor W Wiggins product page (wwiggins.co.nz/products/sioen-aqualite-pvc-d2360) and FashYas distributor news (new-product post dated 2026-07-05) list the full Aqualite D2360 specifications. Sioen’s corporate site (sioen.com) confirms its technical-textile and maritime positioning.