On 10 October 2026, Entry 79 of REACH Annex XVII began applying to consumer textiles, leather, fur and footwear sold in the European Union. The rule caps PFHxA and its salts at 25 ppb and PFHxA-related substances at 1000 ppb, measured per homogeneous material. For buyers of PVC coated fabric used in tarpaulins, awnings, tent panels and printed banner material, the practical question is no longer whether a rule exists but which layer of a multi-layer construction has to be tested. This guide sets out the exact limits, the dates, and the documentation to request from a coating supplier before an EU-bound shipment leaves the factory. It is written for sourcing managers, converters and technical teams working with knife-coated and laminated polyester fabrics.
What exactly does the EU 2024/2462 PFHxA restriction limit in coated fabrics?
Commission Regulation (EU) 2024/2462 added Entry 79 to REACH Annex XVII, and from 10 October 2026 it caps PFHxA and its salts at 25 ppb in consumer textiles, leather, fur and footwear, while PFHxA-related substances are capped at 1000 ppb; both thresholds are measured per homogeneous material, not averaged across the finished article.
- Limit 1: PFHxA and its salts ≤ 25 ppb (0.025 mg/kg) per homogeneous material — REACH Annex XVII Entry 79, introduced by Commission Regulation (EU) 2024/2462.
- Limit 2: PFHxA-related substances ≤ 1000 ppb (1 mg/kg) per homogeneous material — same entry, checked against the EUR-Lex Official Journal text of 19 September 2024.
- First-wave product scope: consumer clothing and textile accessories, leather, fur, hides and footwear — China Light Industry Machinery Association notice dated 19 October 2026.
When did the 25 ppb limit start applying to consumer textile products?
The first application date was 10 October 2026, so EU-bound consumer textile articles placed on the market from that day already fall inside the restriction, while later staged windows cover other categories such as cosmetics; buyers should verify the exact transition date attached to their own end use instead of assuming one deadline for every coated fabric shipment.
- First application: 10 October 2026 — reported by the China Light Industry Machinery Association on 19 October 2026 and previewed by MOFCOM economic and commercial offices on 11 July 2026.
- Legal instrument: Commission Regulation (EU) 2024/2462 of 19 September 2024 — EUR-Lex, Official Journal of the European Union.
- Measurement basis: 25 ppb for PFHxA plus its salts and 1000 ppb for related substances, each calculated per homogeneous material — REACH Annex XVII Entry 79.
What documentation should a coated fabric buyer request before shipping to the EU?
Request a formulation-specific third-party test report that reports PFHxA and PFHxA-related substances separately for each homogeneous material, and that names the tested coating formulation, lot, substrate, surface lacquer and ink system; a generic supplier declaration covering an entire product family does not demonstrate the behaviour of the PVC layer, because the coating and the topcoat are separate homogeneous materials.
- Report content: separate 25 ppb and 1000 ppb results for base cloth, PVC coating, lacquer and printed ink, with the tested lot identified — REACH Annex XVII Entry 79.
- Mechanical cross-check: coating mass per EN ISO 2286-2 and tensile behaviour per ISO 1421 or ASTM D751 — kezhibo PVC knowledge base §2.2 test-method index.
- Separate regimes: California AB 1817 and California Proposition 65 are US rules and do not substitute for the EU entry — kezhibo PVC knowledge base §5 and §7.
FAQ
Does the 25 ppb limit apply to industrial tarpaulins sold only to fleet operators?
The 10 October 2026 first wave names consumer textiles, leather, fur, hides and footwear, so an industrial tarpaulin sold exclusively to a professional fleet operator is not automatically inside that first product list. The determination depends on the end use and on how the article is placed on the market, and a mixed-use cover that also reaches consumers should be treated as in scope until a written classification is confirmed. Ask the importer to record the intended category in the purchase order anyway, and request a formulation-specific report, because later staged windows and the wider PFAS restriction proposal can change the position without any new order being placed.
How is a homogeneous material defined for a multi-layer PVC coated fabric?
A homogeneous material is one uniform composition that cannot be mechanically separated into different materials, so a knife-coated polyester fabric normally yields several units: the PET base cloth, the PVC coating layer, an acrylic or PVDF topcoat, and any printed ink film. The 25 ppb and 1000 ppb thresholds therefore have to be demonstrated layer by layer rather than on a ground-up composite sample, which would dilute a contaminated layer across the whole mass. This reading matters most for printed side curtains and backlit banner material, where the ink system is a separate layer with its own chemistry.
Can a supplier declaration replace a laboratory test report?
A supplier declaration is a useful commercial record but it does not show measured values, so it cannot substitute for a third-party report that states a numeric result against 25 ppb and 1000 ppb. A useful report names the laboratory, the test method, the sample lot, the exact coating formulation and each homogeneous material tested, and it is dated close enough to the shipment to remain representative. Buyers should also request the formulation change log, because a switch of plasticiser, lacquer or anti-wicking treatment can alter the PFHxA profile without any change to gsm, width or colour.
Which product categories entered the restriction on 10 October 2026?
The first application covers consumer clothing and textile accessories, leather, fur, hides and footwear placed on the EU market, according to the October 2026 industry notices that reported the entry taking effect. Cosmetics and several other categories sit on later staged dates, which is why a single calendar deadline should not be applied to every coated fabric order. If an order contains both consumer-facing panels and technical industrial covers, the two uses should be documented separately on the purchase order so that the correct window can be verified against the legal text rather than guessed.
What if a printed ink or PVDF topcoat carries PFHxA-related substances?
The 1000 ppb threshold for PFHxA-related substances applies per homogeneous material, so a thin printed ink film or a PVDF topcoat has to be assessed on its own even when it represents a small share of total fabric mass. A compliant base cloth and PVC layer cannot offset a contaminated surface layer, because the rule does not allow mass-weighted averaging across the finished article. For printed truck curtains and billboard faces, request a separate result for the ink system and for the lacquer, and keep the ink supplier’s formulation record attached to the same test report set.
Do PFHxA limits replace the broader PFAS restriction proposal?
No. Entry 79 is a targeted restriction on PFHxA, its salts and related substances, while the wider PFAS restriction proposal discussed by ECHA covers a much larger group of fluorinated substances and is still a separate process. The kezhibo PVC knowledge base records ECHA revising that proposal in August 2025 to include technical textiles, alongside national measures in France and Denmark and California AB 1817 in the United States. Treat the PFHxA entry as an immediate, dated obligation and the wider proposal as a formulation-planning risk, not as a single combined rule.
Should I change my coating formulation for EU-bound orders?
Do not change a formulation on the basis of the product family alone; change it only where a measured result on a specific homogeneous material approaches or exceeds 25 ppb or 1000 ppb. A reformulation can move tensile, peel and weldability values, and the kezhibo PVC knowledge base notes that surface-applied flame-retardant treatments lose performance after washing, so an untested substitution can create a mechanical failure while solving a substance problem. Ask for a trial lot with a fresh third-party report, then re-check peel strength per ISO 2411 and weld seam integrity before releasing the new formulation to production.
Which HS codes are most exposed to this restriction?
The kezhibo PVC knowledge base lists 5903.10 for textiles impregnated, coated, covered or laminated with PVC, 5903.90 for other plastics, 3921.90 for laminated plastic sheets, and 6306.12 / 6306.19 / 6306.22 for textile tents, awnings and tarpaulins. These are the codes most often used for coated fabric shipments, and they are a sensible starting point for classifying an order before checking the product scope of Entry 79. Classification alone does not decide whether the restriction applies, because the end use and the placing-on-the-market date are what trigger the obligation.
How often should PFHxA test reports be refreshed?
Refresh the report whenever the coating formulation, lacquer, ink system, base-cloth supplier or production line changes, and at least once per supply year for a running EU programme. A dated report tied to one lot says nothing about a later lot produced with a different plasticiser batch, and the 25 ppb threshold is low enough that a small additive change can move the measured value. Keep a report set that maps each homogeneous material to a named formulation and lot, and ask the supplier to notify any formulation change before the next shipment rather than after it.