TL;DR — INEOS CIRC-ADD in 3 Bullet Points
Starting in October 2026, INEOS Inovyn’s CIRC-ADD is a three-year collaborative project focused on recovering and valorising additives, mineral fillers, and metals extracted from PVC waste containing legacy additives — materials currently landfilled or burned because their additive packages prevent straightforward recycling (source). CIRC-ADD builds on two completed Project Circle successes: CIRC-PVC (2025, construction waste) and DISSOLV (2026, flooring/tarpaulin/carpets). The consortium — ROVI-TECH, Revatech, Revalio, Centexbel, Université libre de Bruxelles, University of Liège, Ghent University — targets the European PVC value chain, supporting industrial deployment of advanced recycling technologies by 2030.
Why Legacy Additives Are the Missing Piece in PVC Recycling
Most PVC recycling today is mechanical: shredding, sorting, melting, and re-extruding the plastic. This works well for relatively clean post-consumer bottles or pipe scraps, but breaks down for PVC containing legacy additives — organotin stabilizers, certain phthalate plasticizers, lead-based pigments, and brominated flame retardants that were phased out in previous decades but remain in long-lived products like roofing membranes, electrical cables, and older tarpaulins.
Advanced PVC recycling — dissolution, gasification, and pyrolysis — can break the PVC polymer chain and recover valuable feedstocks. But the co-products from these processes (additives, mineral fillers like calcium carbonate, metals from pigments and stabilizers) are currently underutilized or treated as waste. CIRC-ADD’s mission is to develop the separation, purification, and reprocessing steps that turn these co-products into saleable materials:
- Legacy additives → recovered and used as raw materials for new PVC formulations or exported to specialty chemical manufacturers.
- Mineral fillers (CaCO₃, talc) → purified and reused in paper coating, paint formulation, or new PVC compounds.
- Metals (lead, cadmium, organotin) → recovered via hydrometallurgical processes and fed back to primary metal refining.
Project Circle Timeline — CIRC-PVC → DISSOLV → CIRC-ADD
| Project | Status | Waste Stream Focus | Key Outcome |
|---|---|---|---|
| CIRC-PVC | Completed 2025 | Construction & demolition PVC waste | Collection, sorting, logistics validated; high-quality recycled PVC (rPVC) produced |
| DISSOLV | Completed 2026 | Flooring, tarpaulins, carpets | Advanced dissolution pilot demonstrated; legacy additives effectively removed; closed-loop for plastisol products |
| CIRC-ADD | Launches Oct 2026 (3-year) | Additives, fillers, metals from all PVC waste streams | Recovery & valorisation processes for co-products of advanced recycling |
What CIRC-ADD Means for PVC Tarpaulin and Coated Fabric Recycling
DISSOLV already demonstrated that PVC tarpaulins — one of the most challenging waste streams because of their multi-layer construction (PVC coating on polyester scrim) — can be recycled via advanced dissolution technology. CIRC-ADD takes that a step further: when those tarpaulin products contain legacy additives (common in tarpaulins manufactured before 2010), CIRC-ADD will recover those additives rather than destroying them.
This is especially relevant for industrial PVC tarpaulins that are produced in Europe and exported globally — when they reach end-of-life, the recovered additives could be repatriated to European PVC resin compounds, creating a truly circular system. At kezhibo, we supply heavy-duty PVC tarpaulin and PVC coated fabric for industrial applications, and we actively track these recycling technology developments to advise customers on end-of-life planning for their tarpaulin inventory.
Consortium Partners — Who’s Involved
CIRC-ADD brings together nine organizations spanning recycling technology, waste treatment, sorting, water treatment, and academia:
- INEOS Inovyn (project lead) — Europe’s largest PVC producer
- ROVI-TECH — Specialized PVC recycling technology provider
- Revatech — Water treatment and separation processes
- Revalio — Co-product valorisation and market development
- Centexbel — Belgian textile and polymer research center (DISSOLV veteran)
- Université libre de Bruxelles (ULB-4MAT) — Materials science and characterisation
- University of Liège (PEPs) — Polymer engineering and processing
- Ghent University — Industrial sustainability and LCA methodologies
Industry Context — Why This Matters in 2026
The European PVC industry’s VinylPlus 2030 Commitment was revised in mid-2026 following a comprehensive mid-term review. The revised framework maintains a target of using at least one million tonnes of recycled PVC in new products by 2030 (source). CIRC-ADD’s additive recovery technology is a critical enabler for that target — without recovering legacy additives, the quality of recycled PVC from complex waste streams will remain capped.
INEOS Inovyn’s broader Project Circle ecosystem already operates two pilot plants in Jemeppe-sur-Sambre, Belgium, where INEOS Inovyn’s main R&D center is located. These pilot plants draw on Vinyloop™ technology experience and will be scaled as CIRC-ADD’s 3-year project progresses. The company’s stated goal: “to make all PVC waste recyclable and aim to have our first industrial unit ready by 2030” (source).
What Buyers and Specifiers Should Do Now
For companies that source or specify PVC products — tarpaulins, geomembranes, roofing membranes, coated fabrics — here’s what CIRC-ADD signals:
- Ask about recycling compatibility — When procuring industrial PVC products, ask suppliers whether they use legacy additives that would require advanced recycling.
- Track the 2030 timeline — By 2029/2030, expect advanced recycling facilities to become operational in Europe. This may influence supply chain decisions for large-scale procurement.
- Review end-of-life plans — If your organization stores or manages PVC inventory, start tracking product age to identify which items are likely to require advanced recycling approaches at disposal.
Sources & Further Reading
- INEOS Inovyn — Project Circle Consortiums: CIRC-PVC, DISSOLV, CIRC-ADD
- VinylPlus Sustainability Forum 2026 — MAKE.IT.HAPPEN. IN EUROPE: Revised 2030 Commitment (June 10-11, 2026)
- INEOS Inovyn — Next-Generation PVC Recycling Pilot Plants in Jemeppe-sur-Sambre