The Short Answer
PVC tarpaulin costs more up front and lasts far longer; PE tarpaulin is cheaper and lighter but wears out in one to three seasons. Choose PVC for anything that must survive multiple weather cycles, and PE for short-term or disposable covers.
Side by Side
| Property | PVC tarpaulin | PE tarpaulin |
|---|---|---|
| Waterproofing | Excellent, welded seams | Good, taped or sewn seams |
| UV resistance | High with stabilisers | Moderate, degrades faster |
| Tensile strength | High | Lower |
| Cost per m2 | Higher | Lower |
| Outdoor lifespan | 3 to 7 years, 10 plus heavy | 1 to 3 years |
| Weldability | Hot-air and RF friendly | Heat weldable but less forgiving |
Where PE Wins
PE is the right call for one-season agricultural covers, temporary dust sheets, and any job where the cover is thrown away after a few months. Its low price and light weight are real advantages at volume.
Where PVC Wins
PVC is the better material for truck covers,集装箱侧帘, tents, awnings, inflatable structures, pond and roof covers, and any project where a failed seam costs more than the saving. Its weldable, high-strength, long-life construction pays back over service life.
Decision Guide
If the cover stays outdoors for more than a year, specify PVC. If it is used once or twice and discarded, PE is fine. When in doubt, calculate cost per service year, not cost per square metre.
Frequently Asked Questions
Which lasts longer, PVC or PE tarpaulin?
PVC tarpaulin typically lasts 3 to 7 years outdoors and often 10 plus for heavy grades, while PE tarpaulin lasts 1 to 3 years. PVC is the better choice for anything that must survive multiple seasons.
Is PE tarpaulin cheaper than PVC?
Yes. PE is lighter and cheaper per square metre, which is why it dominates short-term and disposable covers. For long-term or structural use the lower PVC price per service year usually wins.
Can PE tarpaulin be welded like PVC?
PE can be heat welded but is less forgiving than PVC, and sewn or taped PE seams are common and leak-prone. PVC is the safer choice where waterproof seams matter.