PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric

Durable, versatile 0.9mm PVC-coated fabric for inflatable boats and marine applications.

Specifications

Weight (g/m²) 650 g/m² (typical)
Width (m) 1.5 m (custom)
Thickness (mm) 0.9 mm
Color Custom
Material PVC-coated polyester
Tensile Strength (N/5cm) Warp ≥ 2500 N/5cm, Weft ≥ 2000 N/5cm
Tear Strength (N) Warp ≥ 250 N, Weft ≥ 200 N
Adhesion Strength (N/5cm) ≥ 100 N/5cm
Flame Retardancy Standard Optional
Send Inquiry

Product Details

Pvc Inflatable Boat Fabric 0 9mm Industrial Grade Coated Fabric PVC Inflatable Boat Fabric 0.9mm

Product Introduction

Our PVC inflatable boat fabric 0.9mm is a high-performance coated fabric designed for the demanding marine environment. This material combines a polyester scrim with a robust PVC coating, offering excellent strength, flexibility, and resistance to abrasion, UV, and chemicals. It is the ideal choice for manufacturers of inflatable boats, kayaks, and other watercraft requiring reliable, long-lasting performance.

Technical Parameters

  • Weight: 650 g/m² (typical)
  • Width: 1.5 m (custom widths available)
  • Thickness: 0.9 mm
  • Color: Custom (commonly white, grey, orange, or military green)
  • Material: PVC-coated polyester fabric
  • Tensile Strength: Warp ≥ 2500 N/5cm, Weft ≥ 2000 N/5cm (typical)
  • Tear Strength: Warp ≥ 250 N, Weft ≥ 200 N (typical)
  • Adhesion Strength: ≥ 100 N/5cm (coating to fabric)
  • Flame Retardancy: Optional (meets various standards)

Parameter Analysis

  • Thickness (0.9mm): Provides a balance of flexibility and rigidity, making it easy to handle while offering sufficient puncture resistance for recreational and professional use.
  • Tensile and Tear Strength: The high tensile and tear values ensure the fabric withstands stress from water pressure, impacts, and handling.
  • Adhesion Strength: Strong adhesion between the PVC coating and the polyester base prevents delamination, even under prolonged exposure to water and sunlight.
  • Flame Retardancy: Optional treatment enhances safety in marine environments.

Application Scenarios

  • Inflatable Boats: Ideal for hulls, tubes, and air chambers.
  • Kayaks and Canoes: Lightweight yet durable for paddling crafts.
  • Rafts and Dinghies: Suitable for rescue, leisure, and commercial use.
  • Repair Patches: Used for patching and reinforcing existing inflatable products.

Installation Guide

  1. Cutting: Use sharp tools to cut the fabric to the desired shape, allowing for seam allowances.
  2. Welding: Use hot air welding or high-frequency welding equipment to join panels. Ensure surfaces are clean and dry.
  3. Sealing: Apply PVC adhesive or sealant to seams for extra watertightness.
  4. Valve Installation: Attach valves according to manufacturer instructions, ensuring airtight seals.

Usage Method

  • Inflate the boat to the recommended pressure (usually 0.25–0.3 bar for tubes).
  • Avoid over-inflation, which can stress the fabric.
  • Use on clean water surfaces to minimize abrasion.
  • Follow local regulations for safe operation.

Maintenance Advice

  • Rinse with fresh water after each use in saltwater.
  • Dry thoroughly before storage to prevent mildew.
  • Store in a cool, dry place away from direct sunlight.
  • Inspect regularly for signs of wear or damage.

Repair Tips

  • Clean the damaged area and cut a patch larger than the damaged spot.
  • Apply PVC adhesive to both surfaces, press firmly, and allow to cure.
  • For small punctures, use a repair kit with PVC patches and glue.

Procurement Advice

  • Specify your required width, color, and any special treatments (e.g., flame retardant).
  • Request samples for testing before bulk order.
  • Consider minimum order quantities and lead times.
  • Verify compliance with relevant marine standards if required.

Packaging List

  • Rolls of fabric (typically 50–100 meters per roll)
  • Protective wrapping (kraft paper or PE film)
  • Packing list and quality certificate

FAQ

Q: What is the standard width?

A: Standard width is 1.5 meters, but custom widths are available.

Q: Is this fabric suitable for saltwater use?

A: Yes, it is resistant to saltwater and UV, but rinsing with fresh water after use is recommended.

Q: Can I weld this fabric with a hot air welder?

A: Yes, hot air welding and high-frequency welding are both suitable.

Q: What colors are available?

A: We offer custom colors; common options include white, grey, orange, and military green.

Q: Does the fabric meet any fire safety standards?

A: Flame retardant options are available; please specify your required standard.

This PVC inflatable boat fabric 0.9mm is a reliable choice for manufacturers seeking quality and performance. Contact us for more details and customization options.

Frequently Asked Questions

What is PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric?

PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric is a coated fabric product by Kezhibo New Materials, classified under Coated Fabrics. See the product details on this page for its full specifications.

How can I get a quote for PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.

Leave a Comment

Your email address will not be published. Required fields are marked *