Skip to content

Export Trade Coated Fabric Solutions by Kezhibo

High-performance coated and composite fabrics engineered for global industrial applications.

Specifications

Weight (g/m²) Custom (300-2000 g/m²)
Width (m) Custom (up to 3 m)
Thickness (mm) Custom (0.3-2.0 mm)
Color Custom
Material PVC, PU, or PTFE coated polyester/nylon
Tensile Strength (N/5cm) Custom (1000-5000 N/5cm)
Tear Strength (N) Custom (100-500 N)
Adhesion Strength (N/5cm) Custom (50-150 N/5cm)
Flame Retardancy Standard Custom (meets various standards)
Send Inquiry

Product Details

Export Trade Coated Fabric Solutions By Kezhibo Export Trade Coated Fabric Solutions

Product Introduction

The Export Trade model from Kezhibo New Materials represents our commitment to delivering high-quality coated and composite fabrics for international markets. Designed to meet diverse industrial needs, the Export Trade fabric combines durability, flexibility, and reliability. Whether for protective covers, industrial curtains, or specialized equipment, this fabric is engineered to perform under demanding conditions. Kezhibo’s Export Trade line ensures consistent quality and performance, making it a trusted choice for global buyers.

Technical Parameters

While specific parameters for the Export Trade model may vary based on customization, typical specifications include:

  • Weight: Custom (ranges from 300 to 2000 g/m²)
  • Width: Custom (up to 3 meters)
  • Thickness: Custom (0.3 to 2.0 mm)
  • Color: Custom (any color available)
  • Material: PVC, PU, or PTFE coated polyester or nylon
  • Tensile Strength: Custom (typically 1000 to 5000 N/5cm)
  • Tear Strength: Custom (typically 100 to 500 N)
  • Adhesion: Custom (typically 50 to 150 N/5cm)
  • Flame Retardancy: Custom (meets various standards like BS 7837, NFPA 701)

Parameter Analysis

The Export Trade fabric’s performance is directly influenced by its technical parameters. Weight and thickness affect durability and flexibility, with heavier fabrics offering more strength for heavy-duty applications. Tensile and tear strengths determine the fabric’s ability to withstand stress and punctures, essential for industrial use. Adhesion ensures the coating remains bonded to the base fabric, preventing delamination. Flame retardancy is critical for safety in applications where fire risk exists. Kezhibo can tailor these parameters to meet specific customer requirements, ensuring optimal performance for each use case.

Application Scenarios

The Export Trade fabric is versatile and suitable for a wide range of applications, including:

  • Protective Covers: For machinery, vehicles, and outdoor equipment.
  • Industrial Curtains: Welding curtains, strip curtains, and room dividers.
  • Tarpaulins: For trucks, construction sites, and agriculture.
  • Tents and Shelters: Temporary structures and event tents.
  • Inflatables: Boats, inflatable toys, and advertising displays.
  • Safety Products: Fire blankets, protective clothing, and barriers.

Installation Guide

Proper installation is key to maximizing the performance of Export Trade fabrics. Follow these general guidelines:

  1. Inspect the fabric for any damage before installation.
  2. Use appropriate fasteners such as grommets, ropes, or straps, ensuring they are compatible with the fabric’s thickness.
  3. Avoid sharp edges that could cut or puncture the fabric.
  4. Ensure proper tension when installing to prevent sagging or stress points.
  5. Follow manufacturer instructions for specific applications, such as welding curtains or inflatable products.

Usage Method

The Export Trade fabric is designed for easy handling and use. For most applications:

  • Cutting: Use sharp tools to cut the fabric to desired size.
  • Seaming: Heat sealing or sewing can be used to join pieces, depending on the coating.
  • Cleaning: Wipe with mild soap and water; avoid harsh chemicals.
  • Storage: Store in a cool, dry place away from direct sunlight when not in use.

Maintenance Advice

To extend the lifespan of your Export Trade fabric:

  • Regularly clean the fabric to remove dirt and debris.
  • Inspect for wear and tear, especially at stress points.
  • Protect from UV exposure when possible, as prolonged sunlight can degrade the coating.
  • Repair minor damages promptly to prevent further deterioration.

Repair Tips

If the fabric is damaged:

  • Small punctures: Use a repair patch and adhesive designed for coated fabrics.
  • Tears: Sew or heat-seal the tear, then apply a patch for reinforcement.
  • Coating delamination: Reapply adhesive or use a heat gun to re-bond the coating.
  • For major damage, consult a professional or consider replacing the fabric.

Procurement Advice

When purchasing Export Trade fabric, consider:

  • Application needs: Determine the required strength, flame retardancy, and other specifications.
  • Customization: Kezhibo offers custom colors, widths, and treatments to match your needs.
  • Quality assurance: Ensure the fabric meets relevant industry standards.
  • Sample testing: Request a sample to test before bulk ordering.
  • Lead time: Discuss production and delivery timelines with our sales team.

Packaging List

Each roll of Export Trade fabric is typically packaged as follows:

  • Roll core: 3-inch or 6-inch inner diameter.
  • Wrapping: Protective film or woven bag to prevent damage during transit.
  • Labeling: Product details, batch number, and care instructions.
  • Documentation: Test reports and certificates if required.

FAQ

Q1: Can I get custom colors and widths for Export Trade fabric?

A: Yes, Kezhibo offers full customization for colors, widths, and other specifications.

Q2: What is the minimum order quantity?

A: MOQ varies by product; please contact our sales team for details.

Q3: Does the fabric meet international fire safety standards?

A: We can produce fabric that meets various standards like BS 7837, NFPA 701, and others upon request.

Q4: How should I store the fabric to maintain its quality?

A: Store in a cool, dry place away from direct sunlight and moisture.

Q5: Can I request samples before placing an order?

A: Yes, samples are available for evaluation. Contact us for more information.

—

For more information about the Export Trade model and how Kezhibo can meet your fabric needs, please contact our export team today.

Frequently Asked Questions

What is Export Trade Coated Fabric Solutions by Kezhibo?

Export Trade Coated Fabric Solutions by Kezhibo is a coated fabric product by Kezhibo New Materials, classified under Coated Fabrics. See the product details on this page for its full specifications.

How can I get a quote for Export Trade Coated Fabric Solutions by Kezhibo?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for Export Trade Coated Fabric Solutions by Kezhibo?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does Export Trade Coated Fabric Solutions by Kezhibo meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.

Leave a Comment