PVC 遮阳棚 / 花架膜布 300–600 g/m²

科智博 300–600 g/m² PVC 遮阳棚膜布,PVDF 自洁、抗 UV,适配庭院与商业遮阳。提供哑光/亮光与定制色。

Specifications

Weight (g/m²) 300–600 g/m²
Width (m) 1.5–3.2
Thickness (mm) 0.30–0.55
Color 定制
Material PVC 涂层聚酯(丙烯酸/PVDF 漆)
Tensile Strength (N/5cm) ≥1800 / ≥1600
Tear Strength (N) ≥180
Adhesion Strength (N/5cm) ≥80
Flame Retardancy Standard 可选 B1 / M2
Send Inquiry

Product Details

Pvc Awning Fabric 产品概述

PVC 篷布是科智博以刀刮或压延工艺制成的聚氯乙烯涂层聚酯织物,广泛用于卡车侧帘、货罩、建筑围挡、遮阳与农业覆盖。可按克重、幅宽、颜色与防火等级定制,并支持高频焊接与数码打印。 本文介绍的 PVC 遮阳棚 / 花架膜布 300–600 g/m² 采用PVC 涂层聚酯(丙烯酸/PVDF 漆),标称克重 300–600 g/m²、厚度 0.30–0.55 mm、幅宽 1.5–3.2 m,可按用途定制颜色、防火等级与表面处理。

核心特点

  • PVDF 面层自洁耐候,哑光/亮光可选
  • 抗 UV,长期户外不易黄变
  • 柔软易张拉,适配弧形棚架

技术规格与测试标准

该产品的关键指标如下:拉力 ≥1800 / ≥1600 N/5cm(经/纬),撕裂 ≥180 N,剥离(涂层粘合)≥≥80 N/5cm,阻燃等级 可选 B1 / M2。科智博可提供对应标准的第三方实测报告(如 EN 13501、NFPA 701、EN 12641-2、REACH 等),建议按安装地现行法规核对防火与力学下限后再报价与签约。

主要应用场景

  • 庭院遮阳棚与花架顶
  • 商业外摆与连廊顶棚
  • 阳台与窗户外遮阳

为什么选择科智博新材料

  • 工艺路线透明:主动告知刀刮 / 压延 / 冷贴差异与价差,按终端用途选型而非盲目堆料。
  • 第三方检测报告:可按 EN 13501、NFPA 701、EN 12641-2、REACH 等标准核对实测数据,证书编号可查。
  • 质保承诺:抗 UV 不脆化 5–7 年,提供白纸黑字质保函,附每卷质检卡与批次色差控制。
  • 小批量快反:首单 MOQ 低至 1000㎡/单花色,A4 样片免费、3 个工作日内寄出。
  • 数码打印兼容:提供 UV / 溶剂 / 乳胶三种墨水的附着力测试数据,满足喷绘与灯箱需求。
  • 交期保障:PI 写入逾期每周赔付 0.5% 货值(上限 5%),配合生产进度周报与车间视频。

定制与询价

如需定制克重、幅宽、颜色、透光率或防火等级,请通过本页询价表单提交用途与数量。科智博销售团队将基于 FOB / CIF 双报价反馈价格与交期,并支持 OEM / ODM 与第三方检测协作。

Frequently Asked Questions

What is PVC 遮阳棚 / 花架膜布 300–600 g/m²?

PVC 遮阳棚 / 花架膜布 300–600 g/m² is a coated fabric product by Kezhibo New Materials, classified under PVC 篷布. See the product details on this page for its full specifications.

How can I get a quote for PVC 遮阳棚 / 花架膜布 300–600 g/m²?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC 遮阳棚 / 花架膜布 300–600 g/m²?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC 遮阳棚 / 花架膜布 300–600 g/m² meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.