Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water

Durable and flexible lining solutions for ponds, gardens, and water features.

Specifications

Weight (g/m²) Custom
Width (m) Custom
Thickness (mm) Custom
Color Black, green, or custom
Material PVC-coated polyester or polyethylene
Tensile Strength (N/5cm) High (customizable)
Tear Strength (N) High (customizable)
Adhesion Strength (N/5cm) Excellent
Flame Retardancy Standard Optional
Send Inquiry

Product Details

Pond Garden Liner Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water

PVC geomembrane: flexible impermeable sheet for containment barriers — fish ponds, aquaculture, landfills, tailings ponds, drinking water tanks, biogas digesters, agricultural canals. Thickness 0.5–1.5 mm; 0.5–0.75 mm for ponds/agriculture, 0.75–1.5 mm reinforced for landfills and potable water. Weldability is critical for leak-free installations.

Technical Specifications

Application Thickness Standard Key property
Pond / agricultural liner 0.5 mm (20 mil) ASTM D7176 pH 2–12 resistant, UV-stabilized
Landfill liner / cover 0.75 mm (30 mil) ASTM D7176 / GRI-GM17 Chemically resistant, weldable
Potable water tank (reinforced) 1.0–1.5 mm GRI-GM17 + NSF/ANSI 61 Drinking-water certified
Biogas digester 0.75–1.5 mm reinforced Custom Gas-tight, biogas-resistant

Market Compliance & Import Considerations

Region Key standard
Europe REACH phthalates/lead; NSF/ANSI 61 if drinking-water contact; HS 5903.10.90 ≈ 8%
USA ASTM D7176 (PVC geomembrane); GRI GM15/GM34 (PVC-EIA); NSF/ANSI 61; HS 5903.10.15 = DUTY FREE

Typical Applications

  • Aquaculture & fish pond liners
  • Drinking water tanks & reservoirs
  • Landfill covers & leachate containment
  • Mining tailings ponds
  • Biogas digester covers
  • Agricultural irrigation canals

How to Select the Right Specification

Small backyard pond 0.5 mm (20 mil) — ASTM D7176, UV-stabilized
Large aquaculture reservoir 0.5–0.75 mm, thicker for continuous UV exposure
Municipal / hazardous landfill Reinforced 0.75–1.5 mm / GRI-GM17, leak-detection compatible
Drinking water storage Reinforced 1.0–1.5 mm / NSF/ANSI 61 certified
Strong solvents / hydrocarbons Switch to PVC-KEE / PVC-EIA or HDPE — consult engineer before quoting

Welding & Installation

NOTE PVC geomembrane MUST use hot-air / heat-wedge / RF / solvent welding. NOT extrusion welding. Weld overlap: 100–150 mm.

Procurement Checklist

  • Specify: tensile + tear + peel requirements, fire rating per local code, surface finish (PVDF/acrylic/matte), print ink compatibility
  • All values are industry-typical ranges — we provide third-party lab test reports with every batch
  • Import tariffs & anti-dumping change frequently — verify the latest WTO schedule before pricing
  • Contact [email protected] with your spec requirements and target market for a quick quotation

Quality Assurance and Customization

Every Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water is produced under ISO 9001-controlled processes and tested to ASTM D751 for tensile, tear, and adhesion performance. Typical properties include a basis weight around Custom g/m² and a PVC-coated polyester or polyethylene construction selected for stable welding and long service life. KeZHiBo offers custom widths, colors, and surface treatments—anti-fungal, anti-static, or FR-rated—with third-party inspection available on request, supporting both OEM volumes and project-specific specifications from prototype to delivery.

Frequently Asked Questions

What is Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water?

Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water is a coated fabric product by Kezhibo New Materials, classified under Pool Liner. See the product details on this page for its full specifications.

How can I get a quote for Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does Pond & Garden Liner: Heavy-Duty Waterproof Membrane for Ponds & Water meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.