Kezhibo Industrial Fabric Geomembrane Kezhibo Industrial Fabric – Geomembrane 0.5mm (20mil)
Product Introduction
This Industrial Fabric model, the Geomembrane 0.5mm (20mil), is a high-quality PVC geomembrane designed for reliable containment in pond and agricultural applications. Manufactured by Kezhibo New Materials, this 0.5mm thick membrane provides an effective barrier against water seepage, ensuring efficient water management and environmental protection.
Technical Parameters
- Thickness: 0.5mm (20mil)
- Test Standard: ASTM D7176
Parameter Analysis
The 0.5mm thickness (20mil) strikes a balance between flexibility and durability, making it suitable for a variety of lining projects. The ASTM D7176 standard ensures consistent quality and performance, covering key properties such as tensile strength, tear resistance, and puncture resistance. This specification guarantees that the geomembrane meets industry benchmarks for reliability.
Application Scenarios
This Industrial Fabric is ideal for:
- Pond liners (fish ponds, decorative ponds)
- Agricultural irrigation reservoirs and canals
- Water storage and containment systems
- Secondary containment for agricultural chemicals
Installation Guide
- Prepare the subgrade: ensure the surface is smooth, free of sharp objects, and compacted.
- Unroll the geomembrane and allow it to relax to reduce wrinkles.
- Position panels with sufficient overlap (typically 10-15 cm) for seaming.
- Use appropriate welding or adhesive methods as recommended by Kezhibo for seam integrity.
- Inspect all seams and repair any defects before backfilling or filling with water.
Usage Method
- Handle with care to avoid punctures during installation.
- For pond lining, anchor the edges in trenches to prevent slippage.
- Avoid dragging sharp tools over the membrane surface.
Maintenance Advice
- Regularly inspect for damage, especially after heavy rains or seasonal changes.
- Keep the membrane clean from debris and vegetation that could cause stress.
- Monitor water levels to prevent overstretching.
Repair Tips
- Clean the damaged area thoroughly.
- Cut a patch of the same material larger than the damaged area.
- Use a heat welder or compatible adhesive to bond the patch, ensuring a watertight seal.
- Test the repair with water pressure if possible.
Procurement Advice
- Determine the required area and add 5-10% for overlaps and waste.
- Choose the appropriate thickness based on your project needs; 0.5mm is suitable for low-risk applications.
- Request a sample to verify quality before bulk ordering.
Packaging List
- Rolls of Geomembrane 0.5mm (20mil) (length per roll depends on order)
- Installation manual (if provided)
- Quality certificate
FAQ
Q: What is the thickness of this geomembrane?
A: The thickness is 0.5mm (20mil).
Q: Is this product suitable for fish ponds?
A: Yes, it is commonly used for pond lining, including fish ponds.
Q: What standard does this product meet?
A: It is tested according to ASTM D7176.
Q: Can I install it myself?
A: Yes, with proper preparation and following the installation guide, DIY installation is possible for simple projects.
Q: How do I repair a tear?
A: Clean the area, apply a patch of the same material, and use heat welding or adhesive to seal it.