Architectural PVC Membrane for Tensile Structures & Facades

Durable, flexible, and fire-retardant membrane for modern architectural tensile structures.

Specifications

Weight (g/m²) 750–1500 g/m²
Width (m) Up to 3.0 m
Thickness (mm) 0.5–1.5 mm
Color White, translucent, or custom RAL
Material Polyester fabric with PVC coating
Tensile Strength (N/5cm) High (custom)
Tear Strength (N) Excellent (custom)
Adhesion Strength (N/5cm) Strong (custom)
Flame Retardancy Standard Meets common standards (e.g., DIN 4102 B1, NFPA 701)
Send Inquiry

Product Details

Architectural PVC Membrane for Tensile Structures & Facades

PVC coated polyester tensile membrane fabric for architectural structures — stadium roofs, canopies, skylights, facades, and pedestrian bridges. Industry grades I–V (800–1,550 gsm); higher grades = heavier base fabric = higher load capacity + longer lifespan. PVDF topcoat is standard for outdoor durability (15–20 year, self-cleaning).

Technical Specifications

Grade Weight gsm Tensile N/5cm (warp/weft) Tear N Light % Lifespan
I 800 3,000/3,000 350/310 — 10–15 yr
II 900 4,400/3,900 580/520 ~8 15–18 yr (PVDF)
III 1,050 5,750/5,100 800/950 8–12 15–18 yr
IV 1,300 7,450/6,400 1,400/1,100 8–12 15–20 yr
V 1,450 9,800/8,300 1,800/1,600 8–12 18–20+ yr

Glass-Fiber Base Option (35+ Year Lifespan)

Base Weight Tensile N/5cm Lifespan
Glass-fiber Grade II 800 gsm 3,500/3,500 35+ yr
Glass-fiber Grade III 1,150 gsm 5,800/5,800 35+ yr
Glass-fiber Grade IV 1,550 gsm 7,500/6,500 35+ yr

Market Compliance & Import Considerations

Region Key standard
Europe EN 13501-1 B-s2,d0 (fire, closed/public); DIN 4102 B1 (Germany common); HS 5903.10.90 ≈ 8%
USA NFPA 701 + ASTM E84 FSI≤25 (Class A); CAN/ULC-S109; HS 5903.10.15 = DUTY FREE

Typical Applications

  • Stadium & sports hall roofs (Grade IV–V)
  • Commercial corridors & pedestrian bridges (Grade II most popular)
  • Canopies at retail, hotels, airports
  • Facade cladding (natural daylighting)
  • Landscape shade sails & sculptural installations

How to Select the Right Specification

Light-load temporary Grade I – 800 gsm
Commercial corridor (most common) Grade II – 900 gsm / PVDF / Anti-wick
Medium-span transit hub Grade III – 1,050 gsm
Large-span stadium / facade Grade IV – 1,300 gsm / Grade V – 1,450 gsm
35+ year landmark Glass-fiber base (≈ 2× price, 35+ yr)
Public building fire EN 13501-1 B-s2,d0 — FR mixed into PVC compound (not surface-coated), ask for accredited lab reports

Procurement Checklist

  • Specify: tensile + tear + peel requirements, fire rating per local code, surface finish (PVDF/acrylic/matte), print ink compatibility
  • All values are industry-typical ranges — we provide third-party lab test reports with every batch
  • Import tariffs & anti-dumping change frequently — verify the latest WTO schedule before pricing
  • Contact [email protected] with your spec requirements and target market for a quick quotation

Quality Assurance and Customization

Every Architectural PVC Membrane for Tensile Structures & Facades is produced under ISO 9001-controlled processes and tested to ASTM D751 for tensile, tear, and adhesion performance. Typical properties include a basis weight around 750–1500 g/m² g/m² and a Polyester fabric with PVC coating construction selected for stable welding and long service life. KeZHiBo offers custom widths, colors, and surface treatments—anti-fungal, anti-static, or FR-rated—with third-party inspection available on request, supporting both OEM volumes and project-specific specifications from prototype to delivery.

Frequently Asked Questions

What is Architectural PVC Membrane for Tensile Structures & Facades?

Architectural PVC Membrane for Tensile Structures & Facades is a coated fabric product by Kezhibo New Materials, classified under PVC Membrane. See the product details on this page for its full specifications.

How can I get a quote for Architectural PVC Membrane for Tensile Structures & Facades?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for Architectural PVC Membrane for Tensile Structures & Facades?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does Architectural PVC Membrane for Tensile Structures & Facades meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.