PVC Oil Boom Containment Fabric 610–900gsm

PVC-coated oil boom fabric with a 1000D 20-30 scrim, 610–900gsm, engineered for oil spill containment barriers and floating boom skins.

Specifications

Weight (g/m²) 610–900gsm
Width (m) Custom
Thickness (mm) Custom
Color Custom
Material PVC-coated fabric
Tensile Strength (N/5cm) Custom
Tear Strength (N) Custom
Adhesion Strength (N/5cm) Custom
Flame Retardancy Standard Custom
Send Inquiry

Product Details

This PVC-coated fabric is produced specifically as skin material for oil booms used in spill containment and floating barrier systems. Built on a 1000D 20-30 scrim and coated to a 610–900gsm weight range, it gives boom fabricators a coated textile that balances mechanical reinforcement with the flexibility needed to wrap floats and tension members. Manufacturers and spill-response equipment suppliers choose it as a durable, weldable outer skin for containment booms.

PVC Oil Boom Containment Fabric

Product Overview and Key Features

The fabric is a scrim-reinforced PVC-coated textile. Each supplied parameter translates into a practical property for oil boom construction:

  • 1000D 20-30 scrim: a 1000 denier base yarn in a 20-30 construction provides the dimensional stability and strength backbone that keeps the boom skin from stretching out of shape under wave and current loading.
  • 610–900gsm weight range: a mid-to-heavy coated weight that supports abrasion resistance and robust handling while remaining flexible enough to conform around boom floats and end connectors.
  • PVC coating: a thermoplastic coating that can be heat-welded and sewn, allowing fabricators to join panels into long boom sections and attach hardware.

Because the material is a coated fabric rather than a rigid panel, it can be folded, rolled and deployed from reels or containers during spill response.

Technical Specifications

Property Value
Material PVC-coated fabric
Scrim / base yarn 1000D 20-30
Weight 610–900gsm
Width Custom
Thickness Custom
Color Custom
Tensile strength Custom
Tear strength Custom
Adhesion Custom
Flame resistance Custom

Only the scrim, weight range and PVC coating are fixed by the supplied data. All other values are confirmed per order against the agreed specification.

Parameter and Performance Notes

The 610–900gsm band is a range, not a single figure: lighter weights within it suit smaller or more portable boom sections where handling ease matters, while heavier weights favor larger, more heavily loaded barriers. The 1000D 20-30 scrim is the reinforcement that carries load through the coating; the PVC coating provides the continuous outer surface. Tensile, tear, adhesion and flame performance depend on the final coating formulation and construction, so they are quoted per project rather than assumed. Contact us for the confirmed data sheet for your chosen weight.

Application Scenarios

  • Floating oil containment booms for harbors, marinas and inland waterways
  • Permanent or rapid-deployment spill response barriers
  • Boom skins over foam or air-chamber floats
  • Secondary containment and exclusion barriers around fuel transfer operations
  • Custom-fabricated boom sections joined by heat welding or sewing

In each case the fabric functions as the flexible outer skin of an oil boom, the layer that contacts the water surface and contains the spill.

Customization and OEM/ODM

As a coated-fabric manufacturer we support OEM and ODM programs. Options that can be discussed for an oil boom order include:

  • Weight selection within the 610–900gsm range
  • Roll width and roll length to suit your cutting plan
  • Color and surface finish
  • Printing or logo marking for branding and identification
  • Packaging and labeling to your logistics requirements

These are available possibilities, not fixed guarantees; final options are confirmed in the order specification.

FAQ

Is this fabric UV resistant? UV performance depends on the coating formulation selected. Please contact us for details on the specification suited to prolonged outdoor exposure.

Can it be heat welded into long boom sections? The PVC coating is a thermoplastic surface, which is why the material is used as weldable and sewable boom skin. We recommend confirming welding parameters with your fabricator.

What is the minimum order quantity and lead time? MOQ and lead time depend on weight, width and customization; contact us for a quotation.

Can I get a sample before ordering? Yes — sample requests can be arranged; contact us with your target weight and application.

Is flame-retardant oil boom fabric available? Flame performance is not fixed in the supplied data; contact us to discuss your requirement.

Frequently Asked Questions

What is PVC Oil Boom Containment Fabric 610–900gsm?

PVC Oil Boom Containment Fabric 610–900gsm is a coated fabric product by Kezhibo New Materials, classified under Industrial Fabrics. See the product details on this page for its full specifications.

How can I get a quote for PVC Oil Boom Containment Fabric 610–900gsm?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC Oil Boom Containment Fabric 610–900gsm?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC Oil Boom Containment Fabric 610–900gsm meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.