Skip to content

PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use

Durable, reflective PVC mesh fabric engineered for high-visibility safety applications and industrial covers.

Specifications

Weight (g/m²) 250–500 g/m²
Width (m) 1.0–2.5 m
Thickness (mm) 0.3–0.8 mm
Color Silver, White, Yellow, Orange, Custom
Material PVC-coated polyester mesh with reflective film
Tensile Strength (N/5cm) 500–1500 N/5cm
Tear Strength (N) 50–200 N
Adhesion Strength (N/5cm) ≥ 30 N/5cm
Flame Retardancy Standard Meets various standards (e.g., BS 5438, EN 13501)
Send Inquiry

Product Details

Pvc Mesh Reflective Fabric High Visibility Coated Mesh For Safety Industrial Use PVC Mesh Reflective Fabric – Product Overview

Product Introduction

PVC mesh reflective fabric is a specialized composite material that combines the strength and flexibility of PVC-coated polyester mesh with retroreflective properties. This fabric is designed to enhance visibility in low-light conditions, making it ideal for safety apparel, traffic cones, barrier nets, and industrial covers. The reflective coating is applied to the mesh surface, providing high-intensity reflection when illuminated by headlights or other light sources.

Technical Parameters

While specific values may vary by manufacturer, typical parameters for PVC mesh reflective fabric include:

  • Weight: 250–500 g/m² (customizable)
  • Width: 1.0–2.5 meters
  • Thickness: 0.3–0.8 mm
  • Color: Silver, white, yellow, orange, or custom
  • Material: PVC-coated polyester mesh with reflective film
  • Tensile Strength: 500–1500 N/5cm (warp and weft)
  • Tear Strength: 50–200 N
  • Adhesion: ≥ 30 N/5cm (coating to base fabric)
  • Flame Retardancy: Meets various standards (e.g., BS 5438, EN 13501)

Parameter Analysis

  • Weight & Thickness: Heavier and thicker fabrics offer greater durability and tear resistance, suitable for heavy-duty applications like truck covers. Lighter versions are more flexible and easier to handle for temporary barriers.
  • Tensile & Tear Strength: High tensile strength ensures the fabric can withstand wind loads and mechanical stress. Tear resistance prevents rips from propagating, crucial for safety nets.
  • Adhesion: Strong adhesion between the PVC coating and the mesh base prevents delamination, extending the product’s lifespan.
  • Flame Retardancy: This property is critical for applications where fire safety is a concern, such as in public spaces or industrial settings.

Application Scenarios

PVC mesh reflective fabric is widely used in:

  • Traffic Safety: Reflective barrier nets, traffic cones, and warning tapes.
  • Industrial Safety: High-visibility vests, safety curtains, and machine guards.
  • Outdoor Covers: Truck tarpaulins, boat covers, and equipment protection.
  • Construction: Scaffolding netting with reflective strips for nighttime visibility.
  • Events & Crowd Control: Temporary fencing and barriers.

Installation Guide

  1. Measure and Cut: Measure the required dimensions and cut the fabric using sharp scissors or a utility knife.
  2. Positioning: Place the fabric so that the reflective side faces the direction of incoming light (e.g., toward traffic).
  3. Fixing: Use grommets, ropes, or hook-and-loop fasteners to secure the fabric. For permanent installations, use stainless steel fasteners to avoid corrosion.
  4. Overlap: When joining multiple pieces, overlap edges by at least 5 cm and use double-stitching or heat sealing for a strong bond.

Usage Method

  • Ensure the reflective surface is clean and free of dust or grease to maintain maximum reflectivity.
  • For safety apparel, the fabric should be worn over other clothing and not obstruct movement.
  • In static applications, check that the fabric is taut to prevent flapping, which can cause wear.

Maintenance Advice

  • Clean the fabric regularly with mild soap and water. Avoid abrasive cleaners that can scratch the reflective coating.
  • Rinse thoroughly and air dry. Do not machine dry or iron.
  • Store in a cool, dry place away from direct sunlight when not in use to prevent UV degradation.
  • Inspect periodically for tears or peeling of the reflective layer; repair or replace as needed.

Repair Tips

  • For small tears, use a PVC repair kit or patch with a heat gun to weld a piece of PVC mesh over the damaged area.
  • If the reflective layer is peeling, apply a clear adhesive designed for PVC to reattach it.
  • For major damage, replace the entire section to ensure safety integrity.

Procurement Advice

  • Specify the required tensile strength, flame retardancy, and reflective performance (e.g., retroreflective coefficient) to the supplier.
  • Request samples to test the fabric under your specific conditions.
  • Verify that the fabric meets relevant safety standards (e.g., EN 471 for high-visibility clothing).
  • Consider UV resistance if the fabric will be used outdoors for extended periods.

Packaging List

  • PVC mesh reflective fabric rolls (as ordered)
  • Product data sheet and safety instructions
  • Optional: Grommets, ropes, or installation accessories (if included)

FAQ

Q1: Is PVC mesh reflective fabric waterproof?

Yes, the PVC coating makes it waterproof, suitable for outdoor use.

Q2: Can it be printed on?

Yes, the PVC surface can be printed with logos or warnings using appropriate inks.

Q3: How long does the reflective property last?

With proper care, the reflective coating can last several years, but it may degrade with prolonged UV exposure.

Q4: Is it available in custom colors?

Yes, most manufacturers offer custom color options for both the mesh and the reflective coating.

Q5: Can it be welded or sewn?

Yes, it can be heat-welded or sewn with heavy-duty thread for joining pieces.

Frequently Asked Questions

What is PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use?

PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use is a coated fabric product by Kezhibo New Materials, classified under Coated Fabrics. See the product details on this page for its full specifications.

How can I get a quote for PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC Mesh Reflective Fabric – High-Visibility Coated Mesh for Safety & Industrial Use meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.

Leave a Comment

Your email address will not be published. Required fields are marked *