Specifications

Weight (g/m²) 280–350 g/m²
Width (m) 150–200 cm
Thickness (mm) 0.35–0.50 mm
Color Custom
Material Canvas + Acrylic Coating
Tensile Strength (N/5cm) ≥ 800 N/5cm
Tear Strength (N) ≥ 40 N
Adhesion Strength (N/5cm) ≥ 10 N/5cm
Flame Retardancy Standard Optional
Send Inquiry

Product Details

Acrylic Coated Canvas Awning Fabric Waterproof Kezhibo Industrial Grade Acrylic Coated Canvas Awning Fabric Waterproof – Product Introduction

Kezhibo New Materials presents our acrylic coated canvas awning fabric waterproof solution, engineered for demanding outdoor applications. This fabric combines a robust canvas base with an acrylic coating that provides superior water resistance, UV stability, and longevity. Ideal for awnings, canopies, and protective covers, our acrylic coated canvas awning fabric waterproof is designed to withstand harsh weather while maintaining a clean, professional appearance.

Technical Parameters

| Parameter | Value |

|———–|——-|

| Weight | 280–350 g/m² (customizable) |

| Width | 150–200 cm (customizable) |

| Thickness | 0.35–0.50 mm |

| Color | Custom (standard: white, beige, green) |

| Material | Canvas base + acrylic coating |

| Tensile Strength | ≥ 800 N/5cm (warp & weft) |

| Tear Strength | ≥ 40 N (trapezoid method) |

| Adhesion | ≥ 10 N/5cm (coating to base) |

| Flame Retardant | Optional (meets local standards) |

Parameter Analysis

The technical parameters of our acrylic coated canvas awning fabric waterproof are carefully selected to ensure optimal performance. The weight range (280–350 g/m²) provides a balance between durability and flexibility, making it easy to handle and install. The width and thickness are customizable to suit various awning sizes and structural requirements. Tensile and tear strengths indicate high resistance to mechanical stress, ensuring the fabric can withstand wind loads and repeated folding. Adhesion strength ensures the acrylic coating remains intact, providing long-lasting waterproofing. Optional flame retardancy adds safety for public spaces.

Application Scenarios

This fabric is versatile and suitable for a wide range of outdoor applications:

  • Residential awnings: Patio covers, window awnings, and door canopies.
  • Commercial canopies: Storefront awnings, restaurant terraces, and outdoor seating areas.
  • Industrial covers: Truck covers, equipment protection, and temporary shelters.
  • Recreational uses: Camping tents, gazebos, and event canopies.

Installation Guide

Proper installation ensures the longevity and performance of the acrylic coated canvas awning fabric waterproof. Follow these general steps:

  1. Measure and cut: Measure the frame or area, and cut the fabric with a margin for hemming and fastening.
  2. Hem and reinforce: Fold and sew hems on all edges, adding grommets or webbing for attachment points.
  3. Attach to frame: Use ropes, straps, or screws to secure the fabric to the awning frame, ensuring even tension.
  4. Tension adjustment: Adjust the tension to prevent sagging and allow water runoff.

Usage Method

Once installed, the fabric requires minimal handling. For retractable awnings, operate the mechanism smoothly to avoid stress on the fabric. For fixed awnings, ensure the slope is sufficient for water drainage. Avoid dragging sharp objects across the surface to prevent punctures.

Maintenance Advice

To extend the life of your acrylic coated canvas awning fabric waterproof, follow these maintenance tips:

  • Clean regularly with mild soap and water; avoid harsh chemicals.
  • Rinse thoroughly to remove soap residue.
  • Allow the fabric to dry completely before retracting to prevent mildew.
  • Inspect seams and coatings periodically for wear.

Repair Tips

Minor damages can be repaired easily:

  • For small tears, use a patch kit designed for canvas or acrylic-coated fabrics.
  • For coating delamination, apply a compatible acrylic sealant.
  • If the fabric is severely damaged, consider replacing the panel.

Procurement Advice

When purchasing acrylic coated canvas awning fabric waterproof, consider the following:

  • Specify your exact dimensions and color requirements.
  • Request samples to verify quality and color accuracy.
  • Inquire about flame retardant options if needed.
  • Order a little extra for seams and adjustments.

Packaging List

Each roll of fabric is packaged as follows:

  • Fabric roll wrapped in protective film.
  • Outer packaging with label indicating model, size, and batch number.
  • Optional: certificates of quality and test reports.

FAQ

Q1: Is this fabric truly waterproof?

Yes, the acrylic coating provides excellent water resistance, making it suitable for outdoor use.

Q2: Can I get custom colors?

Absolutely, we offer custom color matching to your specifications.

Q3: How do I clean the fabric?

Use mild soap and water, and avoid abrasive cleaners.

Q4: Does the fabric resist UV fading?

The acrylic coating includes UV stabilizers to minimize fading over time.

Q5: What is the minimum order quantity?

Minimum order quantity is typically 500 meters, but we can accommodate smaller orders for samples.

For more information or to place an order, contact Kezhibo New Materials today.

Frequently Asked Questions

What is Acrylic Coated Canvas Awning Fabric Waterproof – Kezhibo Industrial Grade?

Acrylic Coated Canvas Awning Fabric Waterproof – Kezhibo Industrial Grade is a coated fabric product by Kezhibo New Materials, classified under Coated Fabrics. See the product details on this page for its full specifications.

How can I get a quote for Acrylic Coated Canvas Awning Fabric Waterproof – Kezhibo Industrial Grade?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for Acrylic Coated Canvas Awning Fabric Waterproof – Kezhibo Industrial Grade?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does Acrylic Coated Canvas Awning Fabric Waterproof – Kezhibo Industrial Grade meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.

Leave a Comment

Your email address will not be published. Required fields are marked *