Skip to content

Drop-Stitch Inflatable Fabric 800gsm 0.9mm

800gsm drop-stitch inflatable fabric at 0.9mm, rated 8–12 psi with 4000 N/5cm tensile — a dependable skin for inflatable toys and lightweight air cushions.

Specifications

Weight (g/m²) 800 gsm
Width (m) Custom
Thickness (mm) 0.9 mm
Color Custom
Material Custom
Tensile Strength (N/5cm) 4000 N/5cm
Tear Strength (N) Custom
Adhesion Strength (N/5cm) Custom
Flame Retardancy Standard Custom
Send Inquiry

Product Details

DWF is an 800gsm, 0.9mm drop-stitch inflatable fabric engineered for pressurized air structures. It is aimed at manufacturers of inflatable toys and lightweight air cushions who need a consistent, high-tensile skin that holds shape under inflation. The core benefit is a balanced build: enough tensile strength (4000 N/5cm) to resist internal pressure, at a weight and thickness that keep packed volume and handling manageable.

Drop Stitch Inflatable Fabric DWF Drop-Stitch Inflatable Fabric 800gsm 0.9mm

Product Overview & Key Features

Drop-stitch fabric is a coated textile in which thousands of internal threads connect two fabric faces, so the panel inflates to a controlled thickness instead of ballooning. DWF is supplied at 0.9mm thickness and 800gsm, a combination that suits low-to-medium pressure inflatables. Each supplied parameter translates into a practical property:

  • 800gsm weight — a mid-weight drop-stitch build that balances strength against packed size and material cost, well suited to lightweight air cushions and inflatable toys.
  • 0.9mm thickness — a thin, flexible panel that forms tight curves and folds more easily than heavy drop-stitch stock, while still providing a defined inflated chamber.
  • 4000 N/5cm tensile — high tensile resistance across the 5cm test width, supporting the panel against internal air pressure during use.
  • 8–12 psi working range — a pressure band typical of recreational inflatables, giving a firm inflated surface without demanding heavy-duty construction.
  • 0.9mm chamber — the drop-stitch thread length sets the inflated panel thickness, so the finished part holds a consistent 0.9mm profile when pressurized.

Technical Specifications

Property Value
Weight 800 gsm
Thickness 0.9 mm
Tensile strength 4000–4000 N/5cm
Working pressure 8–12 psi
Chamber thickness 0.9 mm
Width Custom
Color Custom
Material Custom
Tear strength Custom
Adhesion Custom
Flame resistance Custom

Parameter & Performance Notes

The figures above are the supplied specification for DWF and should be read together rather than in isolation. The 4000 N/5cm tensile value describes resistance across a 5cm strip and is the main indicator of how the panel copes with inflation load. The 8–12 psi range defines the pressure band the fabric is intended for; inflating beyond that band is outside the stated specification and should be avoided unless verified for a specific build. Because the drop-stitch chamber is 0.9mm, the finished inflated panel thickness matches the fabric thickness, so designers can plan profiles directly from the 0.9mm value. Weight (800gsm) and thickness (0.9mm) move together — this is a relatively light drop-stitch grade, which favors portability over maximum rigidity. Tear strength, adhesion, flame performance and base material are not fixed in the supplied data; confirm them for your project before finalizing a construction.

Application Scenarios

DWF is positioned for inflatable toys and lightweight air cushions. In practice, an 800gsm, 0.9mm drop-stitch fabric at 8–12 psi suits recreational inflatables where a firm but portable inflated surface is wanted — for example small inflatable play items, air cushions and similar low-pressure inflatable parts. It is not presented here as a heavy-duty structural or high-pressure drop-stitch material; for those duties, discuss the required pressure and load with our team so the grade can be matched to the application.

Customization & OEM/ODM

DWF can be discussed as a base for customized orders. Available options may include color, roll width, panel weight and thickness within what our lines can produce, surface printing or logo marking, and packaging to suit your production or retail needs. These are possibilities for quotation, not fixed guarantees — final availability, tolerances and minimum order quantities are confirmed per order. Share your target pressure, part geometry and volume, and we will advise what is feasible.

FAQ

  • What pressure is DWF rated for? The supplied working range is 8–12 psi. Stay within this band unless a specific build has been verified.
  • How strong is the fabric? Tensile strength is given as 4000–4000 N/5cm. Tear strength and adhesion are not fixed in the current data — contact us for details on your requirement.
  • Is it UV resistant or flame retardant? Flame performance is listed as Custom; UV and flame options should be confirmed with us for your application and market.
  • Can I order samples or custom colors? Color and width are Custom fields, and samples can be discussed. Contact us for details on sample availability, MOQ and lead time.
  • What is the lead time and MOQ? These depend on specification and order size; contact us for details.

Frequently Asked Questions

What is Drop-Stitch Inflatable Fabric 800gsm 0.9mm?

Drop-Stitch Inflatable Fabric 800gsm 0.9mm is a coated fabric product by Kezhibo New Materials, classified under Industrial Coated Fabrics. See the product details on this page for its full specifications.

How can I get a quote for Drop-Stitch Inflatable Fabric 800gsm 0.9mm?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for Drop-Stitch Inflatable Fabric 800gsm 0.9mm?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does Drop-Stitch Inflatable Fabric 800gsm 0.9mm meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.