Skip to content

PVC 屋面防水膜材

科智博 PVC 屋面防水膜材,热风可焊、外露耐候,B1 阻燃,适合平屋面与光伏车棚防水。

Specifications

Weight (g/m²) 900–1500 g/m²
Width (m) 1.5–2.5
Thickness (mm) 0.80–1.50
Color 灰/定制
Material PVC 防水卷材
Tensile Strength (N/5cm) ≥3500 / ≥3200
Tear Strength (N) ≥350
Adhesion Strength (N/5cm) ≥100
Flame Retardancy Standard B1
Send Inquiry

Product Details

Pvc Roofing Waterproofing Membrane 产品概述

防水膜材是科智博面向建筑与市政防水的 PVC 涂层与高分子膜材,涵盖屋面、地下室、隧道桥梁、泳池与种植屋面,强调可焊、耐根穿刺与长期耐候。 本文介绍的 PVC 屋面防水膜材 采用PVC 防水卷材,标称克重 900–1500 g/m²、厚度 0.80–1.50 mm、幅宽 1.5–2.5 m,可按用途定制颜色、防火等级与表面处理。

核心特点

  • 热风焊接成整体,无明火施工
  • 耐候抗 UV,适配外露屋面
  • 搭接强度高,抗风揭

技术规格与测试标准

该产品的关键指标如下:拉力 ≥3500 / ≥3200 N/5cm(经/纬),撕裂 ≥350 N,剥离(涂层粘合)≥≥100 N/5cm,阻燃等级 B1。科智博可提供对应标准的第三方实测报告(如 EN 13501、NFPA 701、EN 12641-2、REACH 等),建议按安装地现行法规核对防火与力学下限后再报价与签约。

主要应用场景

  • 平屋面与金属屋面防水
  • 厂房与仓储外露顶
  • 光伏车棚防水基层

为什么选择科智博新材料

  • 工艺路线透明:主动告知刀刮 / 压延 / 冷贴差异与价差,按终端用途选型而非盲目堆料。
  • 第三方检测报告:可按 EN 13501、NFPA 701、EN 12641-2、REACH 等标准核对实测数据,证书编号可查。
  • 质保承诺:抗 UV 不脆化 5–7 年,提供白纸黑字质保函,附每卷质检卡与批次色差控制。
  • 小批量快反:首单 MOQ 低至 1000㎡/单花色,A4 样片免费、3 个工作日内寄出。
  • 数码打印兼容:提供 UV / 溶剂 / 乳胶三种墨水的附着力测试数据,满足喷绘与灯箱需求。
  • 交期保障:PI 写入逾期每周赔付 0.5% 货值(上限 5%),配合生产进度周报与车间视频。

定制与询价

如需定制克重、幅宽、颜色、透光率或防火等级,请通过本页询价表单提交用途与数量。科智博销售团队将基于 FOB / CIF 双报价反馈价格与交期,并支持 OEM / ODM 与第三方检测协作。

Frequently Asked Questions

What is PVC 屋面防水膜材?

PVC 屋面防水膜材 is a coated fabric product by Kezhibo New Materials, classified under 防水膜材. See the product details on this page for its full specifications.

How can I get a quote for PVC 屋面防水膜材?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC 屋面防水膜材?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC 屋面防水膜材 meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.