Industrial Fabric Geomembrane 0 5mm 20mil Kezhibo Industrial Fabric Geomembrane 0.5mm (20mil)
Product Introduction
Kezhibo’s Industrial Fabric Geomembrane 0.5mm (20mil) is a high-performance PVC coated fabric designed for demanding lining applications. Manufactured to meet ASTM D7176 standards, this industrial fabric offers a robust solution for ponds and agricultural containment. The 0.5mm thickness provides a balance of flexibility and strength, making it suitable for a variety of ground-contact uses.
Technical Parameters
- Model: Industrial Fabric Geomembrane 0.5mm (20mil)
- Thickness: 0.5 mm (20 mil)
- Standard: ASTM D7176
Parameter Analysis
The 0.5mm thickness (20 mil) is a critical specification for this industrial fabric. It ensures adequate puncture resistance and durability while remaining flexible enough for easy installation. Compliance with ASTM D7176 guarantees consistent quality and performance, making this geomembrane a reliable choice for long-term lining projects.
Application Scenarios
This industrial fabric is ideally suited for:
- Pond liners (decorative, fish, or irrigation)
- Agricultural reservoirs and canals
- Secondary containment for livestock or waste storage
- General ground covers requiring waterproofing
Installation Guide
- Prepare the subgrade: remove sharp objects and ensure a smooth, compacted surface.
- Unroll the geomembrane and allow it to relax in the sun before installation.
- Position the fabric over the area, leaving slack to accommodate ground movement.
- Anchor the edges in trenches or with weights to prevent wind uplift.
- For seams, use approved adhesive or welding techniques as recommended by Kezhibo.
Usage Method
- Ensure the fabric is not punctured by sharp stones or roots.
- Use protective geotextile underlay if the subgrade is rough.
- Avoid dragging heavy equipment directly over the installed geomembrane.
Maintenance Advice
- Inspect regularly for tears or punctures, especially after heavy rains or animal activity.
- Keep the surface clean of debris that could cause wear.
- UV exposure may degrade the material over time; consider covering if long-term sun exposure is expected.
Repair Tips
- Clean the damaged area and dry thoroughly.
- Cut a patch of the same industrial fabric, larger than the damaged area.
- Apply a compatible adhesive or heat weld the patch in place.
- Press firmly and allow to cure before refilling with water.
Procurement Advice
- Confirm the required dimensions and quantity based on your project area.
- Request a sample to verify the 0.5mm thickness and flexibility.
- Check that the product complies with ASTM D7176 for quality assurance.
Packaging List
- Industrial Fabric Geomembrane 0.5mm (20mil) rolls (custom widths and lengths)
- Installation and maintenance manual (provided upon request)
FAQ
Q: Is this industrial fabric suitable for potable water?
A: It is designed for general pond and agricultural use; for potable water, please consult Kezhibo for specific material approvals.
Q: Can this geomembrane be used in cold climates?
A: The 0.5mm PVC fabric can become stiff in very low temperatures; proper installation techniques should be used to avoid stress cracking.
Q: How long does this industrial fabric last?
A: Lifespan depends on UV exposure, installation quality, and maintenance; with proper care, it can last many years.
Q: What is the maximum roll width available?
A: Custom widths are available; please contact Kezhibo for specific options.
Q: Is this product recyclable?
A: PVC materials can be recycled in some facilities; check local regulations.