Specifications

Weight (g/m²) 440–550 g/m² (custom)
Width (m) 1.0–3.2 m (custom)
Thickness (mm) 0.32–0.55 mm (custom)
Color White, black, or custom
Material PVC-coated polyester scrim
Tensile Strength (N/5cm) ≥ 2000 N/5cm (typical)
Tear Strength (N) ≥ 250 N (typical)
Adhesion Strength (N/5cm) ≥ 30 N/5cm (typical)
Flame Retardancy Standard Optional (e.g., NFPA 701, DIN 4102 B1)
Send Inquiry

Product Details

PVC sign cloth is a coated fabric engineered for the advertising and display industry. It provides a smooth, printable surface for high-resolution graphics while maintaining strength and flexibility for long-term indoor and outdoor use. This material is ideal for banner manufacturers, print shops, and event companies seeking reliable media for promotional signs.

Pvc Sign Cloth For Banners Flexible Signage PVC Sign Cloth

Product Overview / Key Features

Our PVC sign cloth is produced by coating a high-tenacity polyester scrim with flexible polyvinyl chloride (PVC) on both sides. This construction yields a dimensionally stable substrate that resists stretching and tearing, ensuring your graphics stay crisp and aligned. The matte or gloss finish can be tailored to your application, and the material accepts solvent, eco-solvent, UV, and latex inks for vibrant color reproduction.

  • Durable coated surface: Resists scratches, moisture, and general wear, extending the life of your signage.
  • High tensile strength: The embedded polyester scrim provides excellent tear resistance for large-format banners and tensioned displays.
  • UV-resistant formulation: Helps prevent fading and embrittlement when used outdoors.
  • Printable on both sides: Allows for double-sided banners and displays.
  • Lightweight and flexible: Easy to handle, fold, and install, yet strong enough for suspended or framed applications.

Technical Specifications

Property Value
Weight 440–550 g/m² (custom available)
Width 1.0–3.2 m (custom available)
Thickness 0.32–0.55 mm (custom available)
Color White, black, or custom
Material PVC-coated polyester scrim
Tensile Strength ≥ 2000 N/5cm (warp and weft, typical)
Tear Strength ≥ 250 N (typical)
Adhesion ≥ 30 N/5cm (typical)
Flame Retardancy Optional (e.g., NFPA 701, DIN 4102 B1)

Parameter / Performance Notes

The values listed above are typical for standard PVC sign cloth. Actual performance depends on the specific formulation and manufacturing process. For applications requiring specific certifications or extreme conditions, please consult our engineers to tailor the product to your needs.

Application Scenarios

PVC sign cloth is widely used for:

  • Advertising banners (indoor and outdoor)
  • Roll-up and pull-up display stands
  • Flags and bunting
  • Trade show graphics
  • Backlit signage
  • Construction site hoardings

Customization & OEM/ODM

We offer customization in color, width, weight, and finish. Printing services and logo application are available upon request. Packaging can be tailored for retail or bulk distribution. Contact us to discuss your specific requirements.

FAQ

How durable is PVC sign cloth?

PVC sign cloth is designed for long-term use. The PVC coating protects the fabric from moisture, abrasion, and UV radiation, making it suitable for outdoor applications lasting several years.

Is PVC sign cloth flame retardant?

Flame retardancy is available as an option. If required, we can produce material that meets standards such as NFPA 701 or DIN 4102 B1. Please specify your requirement when ordering.

Can I print on PVC sign cloth?

Yes, the surface is specially treated to accept a wide range of inks, including solvent, eco-solvent, UV, and latex. We can also provide a pre-print treatment if needed.

What is the minimum order quantity?

MOQ depends on the specific product and customization. For standard white sign cloth, MOQ is typically 500 square meters. For custom colors or finishes, please contact us for details.

Can I get samples before ordering?

Yes, samples are available upon request. Please contact our sales team to arrange for samples.

Frequently Asked Questions

What is PVC Sign Cloth for Banners & Flexible Signage?

PVC Sign Cloth for Banners & Flexible Signage is a coated fabric product by Kezhibo New Materials, classified under coated fabrics. See the product details on this page for its full specifications.

How can I get a quote for PVC Sign Cloth for Banners & Flexible Signage?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC Sign Cloth for Banners & Flexible Signage?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC Sign Cloth for Banners & Flexible Signage meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.

Send Inquiry

No file chosen

Supported: PDF, DOC, DOCX, JPG, PNG, XLS, XLSX. Max 5MB.

Leave a Comment

Your email address will not be published. Required fields are marked *