PVC Container Tarpaulin

Durable, waterproof, and versatile protection for cargo and equipment.

Specifications

Weight (g/m²) 650 g/m²
Width (m) 2.0 m
Thickness (mm) 0.55 mm
Color Custom
Material PVC-coated polyester
Tensile Strength (N/5cm) Warp ≥ 2500 N/5cm, Weft ≥ 2200 N/5cm
Tear Strength (N) Warp ≥ 350 N, Weft ≥ 300 N
Adhesion Strength (N/5cm) ≥ 80 N/5cm
Flame Retardancy Standard Meets standard
Send Inquiry

Product Details

PVC Container Tarpaulin

Product Introduction

PVC container tarpaulins are heavy-duty protective covers made from a polyester scrim coated with polyvinyl chloride (PVC). They are designed to withstand harsh weather conditions and provide reliable protection for goods during storage and transportation. The material offers excellent tensile strength, tear resistance, and waterproofing, making it an ideal choice for container covers, truck covers, and outdoor storage.

Technical Parameters

  • Weight: 650 g/m² (typical)
  • Width: 2.0 m (customizable)
  • Thickness: 0.55 mm (typical)
  • Color: Custom (commonly green, blue, orange)
  • Material: PVC-coated polyester
  • Tensile Strength: Warp ≥ 2500 N/5cm, Weft ≥ 2200 N/5cm
  • Tear Strength: Warp ≥ 350 N, Weft ≥ 300 N
  • Adhesion: ≥ 80 N/5cm
  • Flame Retardant: Meets standard (e.g., BS 7837)

Parameter Analysis

The weight and thickness of the PVC container tarpaulin contribute to its durability and resistance to punctures and abrasions. The high tensile and tear strengths ensure the fabric can withstand heavy loads and wind forces. The adhesion between the PVC coating and the polyester base is critical for long-term performance, preventing delamination. Flame retardant properties enhance safety in industrial environments.

Application Scenarios

PVC container tarpaulins are widely used for:

  • Covering shipping containers and cargo during transit
  • Protecting construction materials and equipment on site
  • Covering trucks and trailers
  • Temporary roofing and shelters
  • Agricultural storage (e.g., hay, grain)
  • Outdoor industrial storage

Installation Guide

  1. Lay the tarpaulin over the load or area to be covered.
  2. Ensure the tarpaulin is centered and evenly distributed.
  3. Secure the edges using ropes, bungee cords, or straps.
  4. For large covers, use grommets or eyelets for tie-downs.
  5. Adjust tension to avoid sagging or flapping.

Usage Method

When using the PVC container tarpaulin, ensure it is properly secured to prevent wind uplift. Use reinforced corners and edges for extra strength. Avoid dragging the tarpaulin on rough surfaces to prevent damage. For repeated use, fold and store properly.

Maintenance Advice

  • Clean the tarpaulin with mild soap and water.
  • Rinse thoroughly and allow to dry completely before storage.
  • Store in a cool, dry place away from direct sunlight to prevent UV degradation.
  • Inspect regularly for tears or wear.

Repair Tips

  • For small tears, use a PVC repair patch and adhesive.
  • For larger damage, consider professional welding or sewing.
  • Clean and dry the area before applying any repair material.

Procurement Advice

When purchasing a PVC container tarpaulin, consider:

  • Required size and weight
  • Color and branding options
  • Flame retardant requirements
  • UV resistance for outdoor use
  • Supplier reputation and quality certifications

Packaging List

  • 1 x PVC container tarpaulin (custom size)
  • Repair kit (optional)
  • User manual (if applicable)

FAQ

Q1: Is the PVC container tarpaulin waterproof?

A1: Yes, the PVC coating provides excellent waterproofing.

Q2: Can I get a custom size?

A2: Yes, we offer custom cutting and sewing to your specifications.

Q3: How do I clean the tarpaulin?

A3: Use mild soap and water, avoid harsh chemicals.

Q4: Is it flame retardant?

A4: Yes, it meets standard flame retardant requirements.

Q5: What is the typical lifespan?

A5: With proper care, it can last several years, depending on usage and exposure.

Frequently Asked Questions

What is PVC Container Tarpaulin?

PVC Container Tarpaulin is a coated fabric product by Kezhibo New Materials, classified under Industrial Fabrics. See the product details on this page for its full specifications.

How can I get a quote for PVC Container Tarpaulin?

Send your requirements — such as weight, width, color and intended application — through the inquiry form on this page. The Kezhibo sales team will reply with pricing and lead time for your specification.

Does Kezhibo offer OEM/ODM customization for PVC Container Tarpaulin?

Yes. Kezhibo provides OEM/ODM services for its coated fabric products and can adjust specifications to match your project requirements. Contact the team to discuss the details.

Is Kezhibo an ISO certified manufacturer?

Yes. Kezhibo operates under an ISO 9001 certified quality management system, as announced in the company news section of this website.

Does PVC Container Tarpaulin meet flame retardancy standards?

Check the "Flame Retardancy Standard" row in the specification table on this page. If a specific fire-rating certificate is required, mention it in your inquiry and Kezhibo will confirm the available options.